نتایج جستجو برای: biological corrosion

تعداد نتایج: 494394  

2017
Zhongying Han Xiaoguang Huang Yinfeng Li

9 In some sour reservoirs and tertiary oil recovery blocks, SO42in solution can cause the corrosion 10 and corrosion fatigue of the sucker rods. In this paper, the corrosion behaviors of super-strength 11 sucker rod FG20 (16Mn2SiCrMoVTiA) steel in the well fluid are investigated by electrochemical 12 measurements, and electron probe micro-analyzer (EPMA) analysis. The results show that FG20 ste...

Journal: :Acta of bioengineering and biomechanics 2013
Barbara Burnat Magdalena Walkowiak-Przybyło Tadeusz Błaszczyk Leszek Klimek

In this work, we performed comparative studies of the effect of surface preparation of Ti6Al4V and Ti6Al7Nb biomedical alloys and the influence of endothelial cells on their corrosion behaviour in PBS (Phosphate Buffered Saline). Two different methods of surface modification were applied - polishing and sandblasting. The polished Ti6Al7Nb alloy was found to have the best resistance against gene...

2015
Ahmad Zaki Hwa Kian Chai Dimitrios G. Aggelis Ninel Alver

Corrosion of reinforced concrete (RC) structures has been one of the major causes of structural failure. Early detection of the corrosion process could help limit the location and the extent of necessary repairs or replacement, as well as reduce the cost associated with rehabilitation work. Non-destructive testing (NDT) methods have been found to be useful for in-situ evaluation of steel corros...

2004
Ying Xiao Srdjan Nešić

In this paper a two-dimensional (2-D) stochastic localized CO2 corrosion model is proposed, which describes the balance of two processes: corrosion (leading to metal loss) and precipitation (leading to metal protection). The model is able to predict localized corrosion of carbon steel in CO2 containing environments. The model uses corrosion rate and surface-scaling tendency predicted by a 1-D m...

2017
F. Mahvash S. Eissa T. Bordjiba A. C. Tavares T. Szkopek M. Siaj

Hexagonal boron nitride (hBN) is a layered material with high thermal and chemical stability ideal for ultrathin corrosion resistant coatings. Here, we report the corrosion resistance of Cu with hBN grown by chemical vapor deposition (CVD). Cyclic voltammetry measurements reveal that hBN layers inhibit Cu corrosion and oxygen reduction. We find that CVD grown hBN reduces the Cu corrosion rate b...

2011
Xuefeng Zhao Peng Gong Guofu Qiao Jie Lu Xingjun Lv Jinping Ou

In this paper, a novel kind of method to monitor corrosion expansion of steel rebars in steel reinforced concrete structures named fiber optic coil winding method is proposed, discussed and tested. It is based on the fiber optical Brillouin sensing technique. Firstly, a strain calibration experiment is designed and conducted to obtain the strain coefficient of single mode fiber optics. Results ...

2018
Haixiang Chen Dejun Kong

An arc-sprayed amorphous Al–Ti–Ni coating on S355 structural steel was processed by laser remelting (LR) at powers of 600, 800, and 1000 W. The surface-cross-sectional morphologies, chemical element distributions, and phase compositions of the as-obtained Al–Ti–Ni coatings were analyzed using a scanning electron microscope (SEM), energy-dispersive spectrometer (EDS), and X-ray diffractometer (X...

2012
Václav Čuba Viliam Múčka Milan Pospíšil

In some cases, a corrosion system may be exposed to radiation field. Most usually, it occurs as a part of atmospheric corrosion, when materials are, besides other factors, exposed also to visible and ultraviolet radiation. Technical significance of corrosion caused by such types of radiation is rather small. On the other hand, metallic materials may be exposed to high energy ionizing radiation ...

2016
Genghua Cao Datong Zhang Weiwen Zhang Wen Zhang

Corrosion behavior of friction stir processing (FSP) WE43 alloy in a simulated body fluid (SBF) was investigated. Micro-galvanic corrosion was the dominated corrosion behavior, and the corrosion resistance of FSP WE43 alloy was improved compared to the cast counterpart. Furthermore, due to the fine-grained and homogeneous microstructure, uniform corrosion morphology was observed on FSP WE43 all...

Journal: :Biofouling 2004
Jason S Lee Richard I Ray Edward J Lemieux Alexander U Falster Brenda J Little

Corrosion of 1020 carbon steel coupons in natural seawater over a 1-year period was more aggressive under strictly anaerobic stagnant conditions than under aerobic stagnant conditions as measured by weight loss and instantaneous corrosion rate (polarization resistance). Under oxygenated conditions, a two-tiered oxide layer of lepidocrocite/goethite formed. The inner layer was extremely tenaciou...