نتایج جستجو برای: tzp matrix
تعداد نتایج: 365313 فیلتر نتایج به سال:
Bioinert ceramics, like alumina and zirconia are used mainly for replacements of bones, hip joints and for dental implants. Partially stabilized zirconia ceramics (PSZ or TZP with 3 mol.% or 5 wt.% Y2O3), appear as perspective bioinert ceramics because of their high strength and corrosion resistance. In order to fabricate complex shapes, it is essential to use a near ...
Nowadays it is possible to produce ceramic parts with solid and complex shapes rapid efficient shaping sintering techniques. In this paper, 3mol% yttria stabilized zirconia (3Y-TZP) dense lattice were shaped by Digital light processing method (DLP) densified conventional (CV) microwave (MW) sintering. 3Y-TZP samples MW sintered up 1550 °C different heating rates (10, 30, 50 °C/min) for the 30 °...
A Strength Behavior Approach for 3Y-TZP Ceramics Dental Implants Based on Finite Element Simulations
This study is based on the numerical simulation of mechanical response yttrium-stabilized zirconia ceramic (3Y-TZP) dental implants as a function their intrinsic geometry and masticatory loads. Samples (n=20) 3Y-TZP ceramics were compacted, sintered at 1500 °C - 2h, characterized by relative density, X-Ray diffraction (XRD), scanning electron microscopy (SEM). The elastic parameters (modulus el...
Objectives Many advantages have been attributed to dental zirconia ceramics in terms of mechanical and physical properties; however, the bonding ability of this material to dental structure and/or veneering ceramics has always been a matter of concern. On the other hand, hydroxyapatite (HA) shows excellent biocompatibility and good bonding ability to tooth structure, with mechanically unstable ...
Nanocrystalline cerium(LV) oxide (CeO2, ceria) particles were produced via the hydrothermal treatment of cerium nitrate hexahydrate with various alkali metal hydroxides (MOH: M = Li, Na, K). Experimental conditions such as [MOH], reaction temperature, and reaction time were studied. Particle morphology as well as size of crystallites was precisely controlled by choice of experimental conditions...
Clinically, fractures are the main cause of computer-aided design and computer-aided manufacturing (CAD/CAM) 3 mol%-yttria-stabilized tetragonal zirconia polycrystal (Y-TZP) all-ceramic dental restorations failure because of repetitive occlusal loading. The goal of this work is to study the effect of test methods and specimen's size on the flexural strength of five ceramic products. Both bi-axi...
Despite the increasing utilization of all-ceramic crown systems, their mechanical performance relative to that of metal ceramic restorations (MCR) has yet to be determined. This investigation tested the hypothesis that MCR present higher reliability over two Y-TZP all-ceramic crown systems under mouth-motion fatigue conditions. A CAD-based tooth preparation with the average dimensions of a mand...
PURPOSE The purpose of this study was to evaluate the effect of nano-structured alumina surface coating on shear bond strength between Y-TZP ceramic and various dual-cured resin cements. MATERIALS AND METHODS A total of 90 disk-shaped zirconia specimens (HASS CO., Gangneung, Korea) were divided into three groups by surface treatment method: (1) airborne particle abrasion, (2) tribochemicalsil...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید