The continuously annealed low-carbon-steel strips from industrial production showed an average aging index of about 30 N/mm². This increase in yield strength caused by the continuous-annealing process was strongly dependent on soaking temperature and time. Whilst optimization overaging parameters use a higher annealing would reduce ageing susceptibility strips, it considered unlikely that its m...