آلیاژ ti-6al-4v در یک کورة اتمسفر کنترل توسط آلیاژ پرکنندة آمورف 1228 stemet با ترکیب شیمیـایی (ti-27zr-14cu-13ni, wt%) لحیم شد. ابتدا کیفیت اتصالات لحیم توسط آزمون اولتراسونیک و با استفاده از روش اندازه گیری ضخامت کراتکرامر برانسون[i] ارزیابی شد. سپس تأثیر زمان و دماهای مختلف بر ریزساختار و خواص مکانیکی بررسی شد. بررسی ریزساختار توسط میکروسکوپ نوری، میکروسکوپ الکترونی روبشی[ii] و بررسی خواص مک...
The effects of surface modification treatments such as shot peening, ion implantation (carbon and nitrogen), surface lubrication (soft coating), laser gas nitriding and various combinations thereof, on the fretting fatigue resistance of Ti-6Al-4V have been investigated. The best of these surface treatments appears to be shot peening. While ion implantation improves the base metal fretting fatig...
در این تحقیق، نانولایه کاربید تانتالوم با ضخامت 500 نانومتر بر روی سطح آلیاژ Ti-6Al-4V با روش رسوب دهی فیزیکی از فاز بخار با پرتو الکترونی به منظور اصلاح سطح زیرلایه، پوشش داده شد. با ارزیابی سختی سطح نمونهها، سختی سطح نمونه اصلاح شده با پوشش کاربید تانتالوم (Ti-6Al-4V/Ta2C) نسبت به نمونه بدون پوشش (Ti-6Al-4V) به عنوان شاهد از HV346 به HV640 افزایش یافت. همچنین با انجام آزمون خوردگی در محلول ...
Nanostructured potassium-incorporated Ti-based oxides have attracted much attention because the incorporated potassium can influence their structural and physico-chemical properties. With the aim of tuning the structural and physical properties, we have demonstrated the wet corrosion process (WCP) as a simple method for nanostructure fabrication using various Ti-based materials, namely Ti-6Al-4...
In this study, corrosion behavior of Ti-6Al-4V titanium alloy joint by friction stir welding with a rotational speed of 375 rpm and a travel speed of 100 mm/min was investigated. The welding procedure was carried out under β-transus temperature that was consisted of equiaxed grains in the stir zone. The corrosion behavior of the welded joint was investigated in 3.5% NaCl solution at temperature...
The durability of Fe-Co thin films bonded on Ti-6Al-4V was studied as a function of layer thickness at ambient temperature. Interface toughness of the thin films was characterized by indentation and analyzed using an interface fracture model. The critical stresses for interface debonding and the fatigue life response of Ti-6Al-4V with and without Fe-Co thin films were evaluated by three-point b...
Polished surfaces of Ti-6Al-4V, the most commonly used titanium alloy, were observed to suffer from hydride growth and associated embrittlement during hydrogen charging, whereas rough suffered no such susceptibility. Direct microscopic analyses recombined bubbles thermal desorption spectroscopy (TDS) revealed that surface roughening promotes recombination atomic molecular hydrogen, in turn, red...
Heat treatments tailored for additive manufactured Ti-6Al-4V can be used to attain desirable microstructures associated with superior mechanical properties. Rapid heat treatments, example, recrystallise the microstructure of laser powder bed fusion (L-PBF) obtain refined and quasi-equiaxed prior-β grains. In this study, we discuss interplay between tensile properties specimens. The influence in...
This work studies the tensile properties of Ti-6Al-4V samples produced by laser powder bed based Additive Manufacturing (AM), for different build orientations. The results showed high scattering of the yield and tensile strength and low fracture elongation. The subsequent fractographic investigation revealed the presence of tungsten particles on the fracture surface. Hence, its detection and im...