In this research, a lithium ion conducting lithium aluminum germanium phosphate (LAGP) glass-ceramic with a formula of Li1.5Al0.5Ge1.5(PO4)3 was synthesized by melt-quenching method and subsequent crystallization at 850 °C for 8 h. The prepared glass-ceramic was characterized using X-ray diffraction analysis (XRD) and field emission scanning electron microscopy (FESEM). The XRD patterns exhib...
A conducting lithium aluminum germanium phosphate (LAGP) glass-ceramic with a formula of Li1.5Al0.5Ge1.5(PO4)3 was synthesized by melt-quenching method and subsequent crystallization at 850 °C for 8 h. The prepared glass-ceramic was characterized using differential scanning calorimetry (DSC), X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), and AC impedance techniqu...
The influence of NaNO2, HNO3 and H2SO4 on the structure and morphology of gamma-alumina was investigated by XRD, BET, SEM and FT-IR spectroscopy. Selected amounts of NaNO2, HNO3 and H2SO4 were added to a solution of aluminum isopropoxide (as a precursor for the boehmite synthesis). The boehmite samples were calcined at 350 and 600 ℃ to form the semi-crystalline high surface area gamma-Al2O3. Th...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید