Data is presented describing the strain-controlled, fully-reversed uniaxial cyclic deformation and fatigue behavior of Ti-6Al-4V specimens additively manufactured via Laser Engineered Net Shaping (LENS) - a Direct Laser Deposition (DLD) process. The data was collected by performing multiple fatigue tests on specimens with various microstructural states/conditions, i.e. in their 'as-built', anne...
Six types of diamond-like carbon (DLC) coatings with zirconium (Zr)-containing interlayers on titanium alloy (Ti-6Al-4V) were investigated for improving the biotribological performance of orthopedic implants. The coatings consist of three layers: above the substrate a layer stack of 32 alternating Zr and ZrN sublayers (Zr:ZrN), followed by a layer comprised of Zr and DLC (Zr:DLC), and finally a...
Biomaterial surface functionalization remains of great interest in the promotion of cell osteogenic induction. Previous studies highlighted the positive effects of porous Ti-6Al-4V and phospholipid coating on osteoblast differentiation and bone remodeling. Therefore, the first objective of this study was to evaluate the potential synergistic effects of material porosity and phospholipid coating...
The fatigue behavior and fracture mechanisms of additively manufactured Ti-6Al-4V specimens are investigated in this study. Three sets of testing samples were fabricated for the assessment of fatigue life. The first batch of samples was built by using Laser-Engineered Net Shaping (LENS) technology, a Direct Energy Deposition (DED) method. Internal voids and defects were induced in a second batc...
The biocompatibility of two different titanium alloys, Ti-6Al-4V ELI and Ti-5Al-2, 5Fe, and pure titanium were evaluated. The results were as follows: 1) Titanium alloys were implanted into the dorsal subcutaneous tissues of the Hartley guinea-pig for 12 weeks, immersed in calf serum or in Ringer's solution for 8 weeks. The surface changes of the titanium alloys were observed by SEM and the che...
Removable osseointegrated titanium mini-implants were successfully used as anchorage devices in orthodontics. The early load is necessary to simplify the mini-implant methodology, but can lead to failure during osseointegration. The Ti-6Al-4V alloy was used instead of commercially pure Ti due to its superior strength. However, the corrosion resistance is low, allowing for metal ion release. The...
In the presented work, formation of anodic oxide film on Ti-6Al-4V ELI (Extra Low Interstitial) alloy in 0.02 M trisodium phosphate (Na
Near-net shape processes, such as laser metal deposition (LMD), offer a unique combination of process flexibility, time savings, and reduced cost in producing titanium alloy components. The current challenge in processing titanium alloys using LMD methods is understanding the complex microstructural evolution as a part is fabricated layer by layer. The microstructure is affected by the repeated...
STATEMENT OF PROBLEM The poor chemical bonding of a denture base resin to cast titanium framework often introduces adhesive failure and increases microleakage. PURPOSE This study evaluated the shear bond strengths of a heat cure denture base resin to commercially pure titanium, Ti-6Al-4V alloy and a cobalt-chromium alloy using two adhesive primers. MATERIAL AND METHODS Disks of commercially...
The attachment of cells to titanium surfaces is an important phenomenon in the area of clinical implant dentistry. A major consideration in designing implants has been to produce surfaces that promote desirable responses in the cells and tissues. To achieve these requirements, the titanium implant surface can be modified in various ways. This research was designed to elucidate the relationship ...