In this work, the experiment was conducted to investigate the effect of temperature and sub-bituminous coal on upgrading nickel laterites ores by carbothermic reduction. The reduction was carried out in the muffle furnace at a temperature ranging of 800-1100 o C. The produced calcine from reduction step was grounded in vibrating mill, mixed with water and passed on a magnetic separator to separ...
Two commercial methods are used for the production of strontium carbonate:1) Direct conversion of Celsetite to strontium carbonate by hot sodium carbonate,2) Carbothermic reduction of celestite with coal followed by water leaching of strontium sulfide(SrS) and its conversion to strontium carbonate.The present study has been made on the carbothermic reduction of celestite ores of Varamin (Iran) ...
Results of reducibility tests of reduction conducted on iron ore pellets with carbon are presented in this work. Work done is centered on reduction kinetics using carbon as reducing agent with conventional heat supply (heat transfer process) compared with reduction kinetics where heat is supplied by microwaves to the whole volume. Ore used in this work is called "Alzada" which has reducibility ...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید