Journal: :international journal of iron & steel society of iran 2013
m. kazazi a. afshar m. sajjadnejad

one of the problems in the case of stainless steels is their low corrosion resistance against pitting corrosionin chloride containing environments, thereby leading to severe damage to industries. in this research, the pitting corrosion of 304 austenitic stainless steel was studied in 3.5% nacl solution at room temperature (25˚c) by performing electrochemical measurements (containing cyclic pola...

2013
Arash Shahryari

The localized corrosion behavior of laser surface melted 304L austenitic stainless steel was studied by potentiodynamic polarization test. The extent of improvement in corrosion resistance was governed by the preferred orientation and the percentage of delta ferrite present on the surface of the laser melted sample. It was established by orientation imaging microscopy that the highest pitting p...

Journal: :JCP 2012
Hong Men Jing Zhang Lihua Zhang

In this paper, the level of corrosion and the corrosion rate of 304 stainless steel induced by sulfatereducing bacteria were studied using electrochemical noise. The noise data were analyzed by time domain and frequency domain combined with the observations of optical microscope. And the corrosion was divided into four categories: passivation, pitting induction period, pitting and uniform corro...

1998
Jack Leifer Philip E. Zapp John I. Mickalonis

Statistical models have been developed to predict the occurrence of pitting corrosion in carbon steel waste storage tanks exposed to radioactive nuclear waste. The levels of nitrite concentrations necessary to inhibit pitting at various temperatures and nitrate concentrations were experimentally determined via electrochemical polarization and coupon immersion corrosion tests. Models for the pit...

2016
Robert E. Melchers Igor A. Chaves Robert Jeffrey Recep Avci

The critical role of manganese sulphide (MnS) inclusions for the initiation of the short-term growth of pitting or localized corrosion of low carbon steels has long been recognized. Classical results show that pitting probability and pitting severity increases with increased sulphide concentration for low carbon steels as a result of magnesium sulphides acting as local cathodes for initiating p...

2003
YuPo J. Lin Edward J. St.Martin James R. Frank Nancy C. Comstock

Government retains for itself, and others acting on behalf, a paid-up, nonexclusive, irrevocable worldwide license and said article to reproduce, prepare derivative works, distribute copies to the public, and perform publicly and display publicly, by or on behalf of the Government. The purposes of this project are to (1) minimize the environmental discharge of hydrocarbons and treatment chemica...

Journal: :Biomaterials 2003
L Tan R A Dodd W C Crone

The understanding of corrosion behavior in NiTi is critical for the devices using this shape-memory alloy. In order to improve the surface properties of NiTi such as corrosion resistance, plasma source ion implantation (PSII) technique was employed with oxygen as incident ions at three levels of implantation dose (5x10(16), 1x10(17) and 3x10(17) ions/cm(-2)). Pitting corrosion and wear-corrosio...

2017
Zixuan Yang Bo Kan Jinxu Li Yanjing Su Lijie Qiao Alex A. Volinsky

Inclusion-induced pitting initiation mechanisms in X70 steel were investigated by scanning electron microscopy, scanning Kelvin probe force microscopy (SKPFM), immersion and electrochemical polarization tests in chloride-containing ion solutions. There are three inclusion types in the X70 steel. Corrosion test results indicated that pitting corrosion resistance of type A inclusion < type C incl...

Journal: :Entropy 2014
Zhi Tang Lu Huang Wei He Peter K. Liaw

The effects of metallurgical factors on the aqueous corrosion behavior of highentropy alloys (HEAs) are reviewed in this article. Alloying (e.g., Al and Cu) and processing (e.g., heat treatments) effects on the aqueous corrosion behavior of HEAs, including passive film formation, galvanic corrosion, and pitting corrosion, are discussed in detail. Corrosion rates of HEAs are calculated using ele...

2012
Mitsuharu Shiwa Hiroyuki Masuda Hisashi Yamawaki Kaita Ito Manabu Enoki

Acoustic emission with near-field detection and optical video microscope monitoring was proposed to investigate the pitting corrosion caused by a small magnesium-chloride droplet. Four types of the detected waveforms were characterized by the wavelet analysis to investigate the corrosion of work-hardened SUS304 stainless steel. After high-activity AE signals observed, the corrosion product shee...