The use of Fe-Al intermetallic compound coatings has been investigated in order to improve the tribological behaviour of carbon tool steel. The coatings were formed by a pack cementation process and subsequently diffusion annealing at 900˚C in an argon controlled atmosphere. The optimum diffusion time was selected on the basis of optimum thickness and tribological behaviour. The microstructure...
In this research, B4C-Ni cermet coating was sprayed on the surface of 4130 steel from B4C and Ni feed-stockpowders using high velocity oxy-fuel (HVOF) method. In order to characterize the tribological behavior of thecoating, ball on disk wear tests were done at the ambient temperature and under the loads of 1, 3 and 5 N.Phase analysis of the coating after spraying was studied ...
Components from 73 failed knee replacements (TKRs) consisting of rotating-platform, mobile-bearing and fixed-bearing implants were examined to assess the patterns of wear. The patterns were divided into low-grade (burnishing, abrasion and cold flow) and high-grade (scratching, pitting/metal embedding and delamination) to assess the severity of the wear of polyethylene. The rotating-platform gro...
New bearing materials for total joint replacement have been explored as the need to improve longevity and enhance performance is driven by the changing demands of the patient demographic. Carbon-reinforced PEEK has demonstrated good wear characteristics in experimental wear simulation in both simple geometry pin-on-plate studies and in total hip joint replacement. Carbon reinforced PEEK CFR-PEE...
the use of fe-al intermetallic compound coatings has been investigated in order to improve the tribological behaviour of carbon tool steel. the coatings were formed by a pack cementation process and subsequently diffusion annealing at 900˚c in an argon controlled atmosphere. the optimum diffusion time was selected on the basis of optimum thickness and tribological behaviour. the microstructure ...
Femoral components of hip replacements are commonly anchored in the femur with bone cement or poly(methyl methacrylate) (PMMA). Wear or fracture of bone cement can lead to loosening of the femoral component, which drastically affects the success and longevity of hip replacements. Self-reinforced composite PMMA (SRC-PMMA) has been previously developed for potential use, as a precoat material for...
In this research, the effect of annealing and aging temperature as well as the effect of quenching media on the microstructure, hardness and dry sliding wear behavior of Ti-6Al-4V alloy has been studied. Cylindrical samples with the diameter of 10 mm and the height of 20mm were solutionized at 930˚C and 1060˚C for 600 seconds and then were quenched in the cold water and in the air. The samples ...
A method is presented to improve the tool life and cutting performance of 300mm diameter tungsten carbide (WC) micro end mills by applying thin (o300nm) fine-grained diamond (FGD) and nanocrystalline diamond (NCD) coatings using the hot-filament chemical vapor deposition (HF-CVD) process. The performance of the diamond-coated tools has been evaluated by comparing their performance in dry slot m...
OBJECTIVE The primary objective was to assess dressing delamination and the ensuing potential consequences during wear and/or removal, as well as the effect of residue remaining in the ulcer following foam breakdown. METHOD In this prospective multicentre study, 32 patients with a grade II or III pressure ulcer were randomised to receive either Allevyn Adhesive or Biatain Adhesive dressing. T...