Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...
Rene-80 nickel-base superalloy as an alloy for production of the jet turbine blades shows high mechanical properties as well as microstructure stability during the high temperature engine operation. In this research, age hardening heat treatment cycle was done on the as-cast Rene-80 superalloy. In the following, microstructure, elemental analysis of phases and macro-hardness of the alloy before...
Joining of Hastelloy C276 nickel-base superalloy to AISI316 Stainless Steel using BNi-2 interlayer performed by transient liquid phase process (TLP) at 1150°C for 5 and 30 minutes. Bonding microstructure was studied using an Optical microscope and a scanning electron microscope (SEM). Vickers hardness test and shear strength test have been used to evaluate the mechanical properties. Microstruct...
Secondary phases, such as laves and carbides, are formed during the final solidification stages of nickel-based superalloy coatings deposited during the gas tungsten arc welding cold wire process. However, when aged at high temperatures, other phases can precipitate in the microstructure, like the γ'' and δ phases. This work presents an evaluation of the powerful optimum path forest (OPF) class...
The application of accurate constitutive relationship in finite element simulation would significantly contribute to accurate simulation results, which play critical roles in process design and optimization. In this investigation, the true stress-strain data of an Inconel 718 superalloy were obtained from a series of isothermal compression tests conducted in a wide temperature range of 1153–135...
A 0.5 μm thick layer of rhodium was deposited on the CMSX 4 superalloy by the electroplating method. The rhodium-coated superalloy was hafnized and aluminized or only aluminized using the Chemical vapour deposition method. A comparison was made of the microstructure, phase composition, and oxidation resistance of three aluminide coatings: nonmodified (a), rhodium-modified (b), and rhodiumand ha...
Reticulated nickel foams were alloyed with 8–9 wt% Al or 14–18 wt% Cr and 5–9 wt% Al in a three-step method consisting of (i) gas-phase deposition of Cr and/or Al onto the struts of a pure Ni foam by pack-cementation at 1000 C; (ii) homogenization at 1200 C to remove concentration gradients and to solutionize the alloyed struts; (iii) aging at 900 C to form c0 precipitates within the struts. Th...
Abstract: In order to predict hot deformation behavior of superalloy nimonic 80A, a back-propagational artificial neural network (BP-ANN) and strain-dependent Arrhenius-type model were established based on the experimental data from isothermal compression tests on a Gleeble-3500 thermo-mechanical simulator at temperatures ranging of 1050–1250 ̋C, strain rates ranging of 0.01–10.0 s ́1. A comparis...
The tribological behavior of a nickel-based single crystal superalloy treated by shot-peening has been investigated. Friction tests under three normal loads and temperatures were carried out based on the ball-on-disk configuration. results showed that coefficient friction (COF) wear rate shot-peened (SP-NBSC) at room temperature nearly 2 times 4 600 ?, respectively. However, there no significan...
Nickel-based superalloys have excellent properties at high temperatures, which makes them appropriate for applications such as turbocharges and aeronautic gas turbines. MAR-M246 is a superalloy developed these kinds of applications. The objective this work was to study the total replacement Ta by Nb in atomic percentage superalloy, regarding oxidation resistance. Although both elements same rol...