نتایج جستجو برای: anode

تعداد نتایج: 11223  

Journal: :journal of advanced materials and processing 0
reza ranjbar department of mining and metallurgical engineering, amirkabir university of technology malek naderi department of mining and metallurgical engineering, amirkabir university of technology arash ghazitabar department of mining and metallurgical engineering, amirkabir university of technology

however, the conventional gold recovery process is cyanidation, due to the recent environmental laws; researchers are looking for alternative methods for the recovery of gold. furthermore, the copper anode slime is one of the most important secondary sources of gold (about 1200 ppm). so, the main objective of the current work is gold separation from copper anode slime as a rich secondary source...

2013
Enrique Quiroga-González Jürgen Carstensen

Cycling tests under various conditions have been performed for lithium ion battery anodes made from free-standing silicon microwires embedded at one end in a copper current collector. Optimum charging/discharging conditions have been found for which the anode shows negligible fading (< 0.001%) over 80 cycles; an outstanding result for this kind of anodes. Several performance parameters of the a...

2016
Hao Deng Dawei Wang Xu Xie Yibo Zhou Yan Yin Qing Du Kui Jiao

In this study, a whole-cell 3D multiphase non-isothermal model is developed for hydrogen alkaline anion exchange membrane (AAEM) fuel cell, and the interfacial effect on the two-phase transport in porous electrode is also considered in the model. The results show that the insertion of anode MPL, slight anode pressurization and reduction of membrane thickness generally improve the cell performan...

Journal: :Physical chemistry chemical physics : PCCP 2011
Hui Lu Liisa Rihko-Struckmann Kai Sundmacher

The spontaneous oscillations of the cell voltage and output power density of a PEMFC (with PtRu/C anode) using CO-containing H(2) streams as anodic fuels have been observed during galvanostatic operating. It is ascribed to the dynamic coupling of the CO adsorption (poisoning) and the electrochemical CO oxidation (reactivating) processes in the anode chamber of the single PEMFC. Accompanying the...

2003
M. S. Dixit

Micro-pattern gas detectors, such as the Gas Electron Multiplier (GEM) and the Micromegas need narrow high density anode readout elements to achieve good spatial resolution. A high-density anode readout would require an unmanageable number of electronics channels for certain potential micro-detector applications such as the Time Projection Chamber. We describe below a new technique to achieve g...

2018
Kangze Shen Ning Lin Tianjun Xu Ying Han Yitai Qian

It is recently demonstrated that amorphous Ge anode shows higher reversible Na-ion storage capacity (590 mA h g-1) than crystallized Ge anode (369 mA h g-1). Here, amorphous GeO x anode is prepared by a simple wet-chemistry reduction route at room temperature. The obtained amorphous GeO x shows a porous hierarchical architecture, accompanied with a Brunauer-Emmett-Teller surface area of 159 m2 ...

2010
Jason B. Siegel Stanislav V. Bohac Anna G. Stefanopoulou Serhat Yesilyurt

In this paper we model and experimentally verify the evolution of liquid water and nitrogen fronts along the length of the anode channel in a Proton Exchange Membrane Fuel Cell operating with a dead-ended anode that is fed by dry hydrogen. The accumulation of inert nitrogen and liquid water in the anode causes a voltage drop, which is recoverable by purging the anode. Experiments were designed ...

2011
Bryan Eichhorn

Title of Document: IN SITU PROCESSING OF PtSn ELECTROCATALYSTS FOR CO TOLERANCE IN PEM FUEL CELLS Robert Utz, Master of Science, 2011 Directed By: Professor Greg Jackson Department of Mechanical Engineering Improved anode CO tolerance is a promising approach for integrating lowtemperature PEM fuel cells with hydrocarbon fuel processors in cost-effective systems for portable and stationary power...

2011
Jian Wang Yuan Chen Lu Qi

With the rapid progress and wide application of Li-ion batteries, commercial graphite anode can not satisfy the increasing demand for higher capacities. Like other anode materials with higher capacities, silicon materials as anodes remain serious problems for their large volume variations and poor cyclabilities during cycling. One of key problem is how to stabilize the performances of Si anode ...

2015
Kazuhiro Yamamoto Nan Qiu Satoshi Ohara

A core-shell anode consisting of nickel-gadolinium-doped-ceria (Ni-GDC) nanocubes was directly fabricated by a chemical process in a solution containing a nickel source and GDC nanocubes covered with highly reactive {001} facets. The cermet anode effectively generated a Ni metal framework even at 500 °C with the growth of the Ni spheres. Anode fabrication at such a low temperature without any s...