Background & Aims: Use of the antioxidants can affect the durability of bond strength in some adhesive systems. This study sought to evaluate the effect of two types of the two step etch and rinse adhesive systems with different solvents on durability of resin composite bonding to the treated dentin with proanthocyanidins. Materials & Methods: In this in vitro experimental study, 80 human mola...
The purpose of this study was to examine the microtensile bond strength of a single-step self-etch adhesive system (Clearfil tri-S Bond and One-Up Bond F Plus) to bovine dentin. Adhesive was applied to a flat dentin surface, and resin composite was bonded according to the manufacturers' instructions. After 24 h storage in distilled water at 37 degrees C, hourglass-shaped specimens were produced...
The present study aimed to evaluate effects of different surface treatments and aging of composite cylinders on bond strength of composite resin repair. Thirty-two composite cylinders were produced and divided into four groups according to type of surface treatment and storage time of composite cylinder and repair. Cylinder surface of control group (Gcontrol) received no treatment before compos...
PURPOSE The aims of this in vitro study were to: (1) compare bond strength of different adhesive systems to primary and permanent dentin using microtensile test; and (2) evaluate the interaction of these materials to primary and permanent dentin by means of scanning electron microscopy (SEM). METHODS Middle-coronal dentin surfaces of 18 exfoliated primary and 18 extracted permanent molars wer...
OBJECTIVE The purpose of this study was to determine the microtensile bond strength of various resin composite/adhesive systems to alumina particle abraded Ti-6Al-4V substrate after aging for 24h, 10 days, and 30 days in distilled water at 37 degrees C. METHODS Four laboratory resin composite veneering systems (Gradia, GR; Solidex, SOL; Ceramage, CER; and Sinfony, SF) were bonded to 25 mm dia...
objective: the aim of this study was to evaluate the microtensile bond strength to sound and caries-affected dentin using single bond and adper prompt-l-pop adhesives. materials and methods: sixteen extracted human molars with carious lesions extended halfway through dentin were ground to expose the caries affected and the surrounding normal dentin. the samples were divided into two groups of e...
The study evaluated the influence of different luting materials on the microtensile bond strength of glass fiber posts to root canal dentin. Thirty extracted maxillary premolars were endodontically treated, and the roots were prepared for post cementation using the FRC Postec system (Vivadent). Two luting materials (Multilink, Vivadent and Clearfil Photo Core, Kuraray) were used in combination ...
OBJECTIVES The purpose of this in vitro study was to evaluate the effect of artificial saliva contamination on microtensile bond strength to pulp chamber dentin. METHODS Clearfil SE Bond (SEB) (Kuraray, JAPAN) adhesive system and Clearfil Photo Posterior (CPP) (Kuraray, JAPAN) composite resin were used. Twenty extracted caries-free human molar teeth were randomly distributed into four groups....
OBJECTIVES To verify the influence of different etching procedures of the post-surface on microtensile bond strength values between fiber posts and composite core materials. METHODS 60 DT Light Posts were divided into 10 subgroups using five different chemical surface treatments and two composite materials to build-up the abutment. Chemical surface treatments including etching with potassium ...