he possibility to obtain sintered material from alkaline basaltic tuffs is demonstrated. The parent rock was milled for 10–15 min, the resulting owder was pressed at 100 MPa and the obtained samples were heat-treated in the range of 1000–1140 ◦C. The sintering behaviour and the phase ormation were studied by pycnometry, dilatometry, DTA, XRD and SEM. The final material was obtained by sintering...