Objectives: Ceramics have advantages such as optimal esthetics and biocompatibility. However, in the oral environment, they are subjected to high levels of stress due to masticatory forces, saliva, thermal changes and alterations of pH, which increase their risk of fracture. Since replacement of these restorations is costly and time-consuming, composite resin is often used for intraoral repair ...
Adhesion is important in many industrial applications including those in the microelectronics industry. Flip-chip assemblies commonly utilize epoxy underfills to promote reliability and the buried interfacial structure of underfills is crucial to device lifetime. Poor adhesion at this interface can cause premature device failure. One method to increase adhesion strength is to plasma treat the s...
the aim of this article is study of tool plunge depth (tpd) effects on mechanical properties of friction stir welding of aa1100 aluminium alloy to a441 aisi steel. for this purpose the 0.1, 0.2, 0.4, and 0.6 mm tpd selected and other welding parameters kept constant. the results shows that the frictional heat increases and stir zone grain size decreases with increasing tpd at both base metals. ...
The aim of this study was to investigate in how far the way the specimen is fixed to the testing device influences the micro-tensile bond strength of adhesives to dentin. Compared to a flat jig, a notched jig enables the specimen to be aligned easier and more accurately perpendicular to the interface, thereby concentrating better the tensile stress at the actual interface. A notched jig yielded...
BACKGROUND An optimum bond strength at the resin-metal interface of a prosthesis is essential to the success of that prosthesis. Silicoater MD and Kevloc are two systems used to increase bond strength at the resin-metal interface. This study investigated the effect that surface pretreatment and chemical shelf life had on the bond strength of silicoated samples and compared the shear bond streng...
In this research, effect of time and temperature of TLP process on the microstructure, mechanical properties and corrosion resistance of CP-Ti to 316L stainless steel joint evaluated. For this purpose pure copper foil with 100 µm thickness was used as interlayer and joining process carried out at 950˚C, 1000˚C and 1050˚C and for 90, 120 and 150 minutes. After the joining process, shear and micr...
Impaction allografting is an attractive procedure for the treatment of failed total hip replacements. The graft-cement-host bone interface after impaction allografting has not been characterized, although it is a potential site of subsidence for this type of revision total hip reconstruction. In six human cadaveric femurs, the cancellous bone was removed proximally and local diaphyseal lytic de...
BACKGROUND Revision arthroplasty often requires anchoring of prostheses to poor-quality or deficient bone stock. Recently, newer porous materials have been introduced onto the market as additional, and perhaps better, treatment options for revision arthroplasty. To date, there is no information on how these porous metals interface with bone cement. This is of clinical importance, since these co...
introduction: debonding is a common cause of failure encountered with fiber-reinforced composite (frc) posts, and usually occurs along the post space-dentin adhesive interface. the aim of this in vitro study is to evaluate the regional push-out bond strength of a fiber-reinforced post system, using two resin cements. materials and methods: in this in vitro study 20 maxillary central incisors we...