نتایج جستجو برای: ceramic laminate
تعداد نتایج: 25713 فیلتر نتایج به سال:
Two-dimensional finite element simulations and experiments are presented to examine the ultrasonic wave propagation behavior in the corner section of CFRP (carbon fiber reinforced plastics) laminate structures. The numerical model consists of a right-angle corner section of CFRP laminate immersed in water and subjected to the ultrasonic wave incidence from its inner or outer side. The anisotrop...
An absorbing material–conductor laminate is widely used for electromagnetic compatibility of electronic circuits at microwave frequencies. Such a laminate when properly designed will exhibit good results in terms of electromagnetic interference and compatibility. In this paper, microwave absorbing materials like 1) Ca-NiTi hexa ferrite composites (Ca (NiTi)x Fe12-2xO19) for x = 0.4, 2) M-Type B...
We have investigated thermal conductivity of graphene laminate films deposited on polyethylene terephthalate substrates. Two types of graphene laminate were studied, as deposited and compressed, in order to determine the physical parameters affecting the heat conduction the most. The measurements were performed using the optothermal Raman technique and a set of suspended samples with the graphe...
Thermoelectric structural materials are potentially attractive for large-scale energy harvesting. Through filler incorporation and unprecedented decoupling of the bulk (laminae) and interfacial (interlaminar interfaces) contributions to the Seebeck voltage (through-thickness Seebeck voltage of a crossply continuous carbon fiber/epoxy composite laminate), this work provides thermoelectric power ...
Aim: The aim of this study was to determine the effect of different luting cements and accelerated artificial aging (AAA) in the fracture resistance of porcelain laminate veneers (PLVs). Materials and methods: A total of 80 disc-shaped specimens were prepared using computer-aided design/computer-aided milling technology from lithium disilicate glass-ceramic blocks. Specimens (0.5 mm thick, 10 m...
Use of direct composite and indirect laminate veneers has been an alternative to metal- and all-ceramic crowns for anterior teeth restorations. Dental traumas are the most common reasons for excessive tissue loss. Treatment options depend on the amount of remaining tissue, the extent of the damage to dental pulp and periapical tissues and the time elapsed before dental treatment. The aim of thi...
Thermo-mechanical models are presented for predicting the time-to-failure of polymer laminates loaded in tension or compression and exposed to one-sided radiant heating by fire. Time-to-failure is defined as the time duration that a polymer laminate can support an externally applied load in a fire without failing. The models predict the temperature rise and through-thickness temperature profile...
Submit Manuscript | http://medcraveonline.com Teeth presenting diastema and misalignment are a common finding in the anterior maxillary dentition, and this fact can strongly affect the appearance of a smile, besides being displeasing for the patients.1 The current literature suggests several approaches for the correction of diastemas and misaligned teeth, such as orthodontic intervention, direc...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید