نتایج جستجو برای: kinetic thermal degradation

تعداد نتایج: 442910  

Journal: :International Journal for Research in Applied Science and Engineering Technology 2020

1996

When wood is exposed to elevated temperatures, changes can occur in its chemical structure that affect its performance. The extent of the changes depends on the temperature level and the length of time under exposure conditions. The changes in chemical structure may be manifested only as reduced strength, and hydroscopic water and volatile oil weight loss. In contrast, very drastic chemical cha...

Journal: :journal of solid mechanics 0
a.r ghasemi faculty of mechanical engineering, department of solid mechanics, university of kashan, kashan, iran m moradi faculty of mechanical engineering, department of solid mechanics, university of kashan, kashan, iran

the principal effects of mass degradation on polymer matrix composites (pmcs) are the decay of mechanical properties such as strength, elongation, and resilience. this degradation is a common problem of the pmcs under thermal cycling conditions. in this article, composite degradation was investigated by measurement of total mass loss (tml) using the taguchi approach. thermal cycling tests were ...

2013
Kelly Ross Amy Leung David Godfrey Giuseppe Mazza

Effective use of crop residues as a source material for the production of energy and biochemicals requires a fundamental understanding of its thermal degradation properties and reaction kinetics. Furthermore, identification of applications for lignin and extractives is essential. Thermogravimetric analysis was used to determine the effect of extractives on the thermal decomposition behaviour of...

2014

Honey is usually subjected to filtration and heating for bottling before commercialization. However, there is no standard procedure available for thermal treatment on honey. Honey is thermally heated at various temperature and duration based on individual experience to prolong the shelf life of honey in the market. The heating methods might decrease the biochemical components such as nutrients,...

2005
Jelena Macan Ivan Brnardić Sebastijan Orlić Hrvoje Ivanković Marica Ivanković

Degradation kinetics of organic-inorganic hybrid materials based on epoxy resin was investigated by thermogravimetric analysis (TGA). The hybrid materials were prepared from diglycidyl ether of bisphenol A (DGEBA) and 3-glycidyloxypropyltrimethoxysilane (GLYMO) polymerised simultaneously by poly(oxypropylene)diamine (Jeffamine D230). Nanometric level of homogeneity in the hybrids was verified b...

Journal: :Acta poloniae pharmaceutica 2014
Przemysław Zalewski Robert Skibiński Judyta Cielecka-Piontek Katarzyna Bednarek-Rajewska

The stability-indicating LC assay method was developed and validated for quantitative determination of cefpirome sulfate (CPS) in the presence of degradation products formed during the forced degradation studies. An isocratic HPLC method was developed with Lichrospher RP-18 column, 5 μm particle size, 125 mm x 4 mm column and 12 mM ammonium acetate-acetonitrile (90 : 10 v/v) as a mobile phase. ...

1999
Margarida C. Vieira

The thermal degradation kinetics of both components of vitamin C, ascorbic acid (AA) and dehydroascorbic acid (DHAA), were determined in a nectar of Cupuac ßu (Theobroma grandi ̄orum) with 25% of pulp and 15% of sugar in water. AA was assayed by HPLC and the results showed that AA degraded into DHAA. A reversible ®rst order model described well the AA degradation data, with an activation energy ...

Journal: :international journal of nano dimension 0
a. mirzaee m.sc. student, department of chemistry, ahar branch, islamic azad university, ahar, iran. p. gharbani 2department of chemistry, ahar branch, islamic azad university, ahar, iran.

the present work is focused on the degradation of 4-chloro-2-nitrophenol in aqueous solution containing nano titanium dioxide, hydrogen peroxide and the combination of nano-tio2/h2o2. the effect of experimental parameters, such as the amount of nano- tio2 concentration of h2o2, initial concentration of 4-chloro-2-nitrophenol and ph on the reaction was investigated. experimental data obtained un...

Journal: :Acta poloniae pharmaceutica 2015
Przemysław Zalewski Piotr Garbacki Judyta Cielecka-Piontek Katarzyna Bednarek-Rajewska Anna Krause

The stability-indicating LC assay method was developed and validated for quantitative determination of cefozopran hydrochloride (CZH) in the presence of degradation products formed during the forced degradation studies. An isocratic, RP-HPLC method was developed with C-18 (250 mm x 4.6 mm, 5 µm) column and 12 mM ammonium acetate-acetonitrile (92:8, v/v) as a mobile phase. The flow rate of the m...