نتایج جستجو برای: rock fracture toughness

تعداد نتایج: 135619  

In this paper, using the Taguchi method, the parameters affecting the toughness of super duplex stainless steels in friction stir welding were optimized. In order to achieve optimal conditions, maximum toughness, the quality characteristic was used as the higher the better. Analysis of Taguchi results showed that in order to achieve optimal conditions in super duplex stainless steel weldments m...

Journal: :Dental materials journal 2012
Haitham Elbishari Nick Silikas Julian Satterthwaite

UNLABELLED The objective of this study was to investigate the correlation between filler size, fracture toughness and voids. Seven model resin composites and one commercial have been used in the study. A single edge notch mould was used to prepare samples (n=8). A selected area of 1mm below and above the notch was scanned with micro CT and then the percentage of voids calculated. A universal te...

2009
MOSTAFA SHAZLY

Recently, a new generation of titanium aluminide alloy named Gamma-Met PX (GKSS, Geesthacht, Germany) has been developed with better rolling and postrolling characteristics. Previous work on this alloy has shown the material to have higher strengths at room and elevated temperatures when compared with other gamma titanium aluminides. In particular, this new alloy has shown increased ductility a...

ژورنال: مجله دندانپزشکی 2018

Background and Aims: Fracture and color change are among the most common causes of clinical failure of resin composite restorations. Therefore, this study aimed to examine the fracture toughness and color changes of 3 Nano-hybrid resin composites in dry and wet conditions. Materials and Methods: Three resin composites were studied. A total of 36 rectangular specimens were prepared for each mat...

Journal: :Engineering With Computers 2022

Abstract In this contribution, a novel framework for simulating mixed-mode failure in rock is presented. Based on hybrid phase-field model fracture, separate variables are introduced tensile (mode I) and shear II) fracture. The resulting three-field problem features length scale parameters mode I II cracks. contrast to the classic two-field approaches, it can thus account different strength of ...

2007
J. W. Foulk R. O. Ritchie

The structural reliability of many brittle materials such as structural ceramics relies on the occurrence of intergranular, as opposed to transgranular, fracture in order to induce toughening by grain bridging. For a constant grain boundary strength and grain boundary toughness, the current work examines the role of grain strength, grain toughness, and grain angle in promoting intergranular fra...

Journal: :The Journal of prosthetic dentistry 2013
Aristotelis Marinis Steven A Aquilino Peter S Lund David G Gratton Clark M Stanford Ana M Diaz-Arnold Fang Qian

STATEMENT OF PROBLEM The fabrication of zirconium dioxide (ZrO2) dental prosthetic substructures requires an extended sintering process (8 to 10 hours) in a conventional oven. Microwave sintering is a shorter process (2 hours) than conventional sintering. PURPOSE The purpose of this study was to compare the fracture toughness of 3 mol % Y2O3-stabilized ZrO2 sintered in a conventional or micro...

2012
F. García Marro R. Kiran Chintapalli

The indentation method has been widely used to measure the fracture toughness in fragile materials due to its simplicity and that only needs of a small sample. However, it is well known that the fracture toughness values obtained by indentation methods can be substantially different from the values obtained from more rigorous methods which are based on a precise knowledge of all parameters invo...

2016
Hongxian Xie Xiaoyan Song Fuxing Yin Yongguang Zhang

The effect of coherency WC/Co phase boundaries on the fracture toughness of the nanocrystalline WC-Co cemented carbides is studied by MD simulation method. The simulation results show that the nanocrystalline WC-Co cemented carbides with coherency WC/Co phase boundaries has higher fracture toughness than that without coherency WC/Co phase boundaries. Moreover, the mechanism of why coherency WC/...

2003

In this chapter some of the standard procedures for delamination testing of unidirectional polymer composites will be examined. The main objective is to explore the possibilities of applying the standard testing methods to interlayer toughened composites and to establish parameters which may influence fracture toughness measurements. Existing standards for mode I and mode II delamination testin...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید