Journal: :Advanced materials 2014
Idan Hod Wojciech Bury David M Karlin Pravas Deria Chung-Wei Kung Michael J Katz Monica So Benjamin Klahr Danni Jin Yip-Wah Chung Teri W Odom Omar K Farha Joseph T Hupp

Electrophoretic deposition (EPD) is used to assemble metal-organic framework (MOF) materials in nano- and micro-particulate, thin-film form. The flexibility of the method is demonstrated by the successful deposition of 4 types of MOFs: NU-1000, UiO-66, HKUST-1, and Al-MIL-53. Additionally, EPD is used to pattern the growth of NU-1000 thin films that exhibit full electrochemical activity.

2013
Anirban Sarkar Theda Daniels-Race

Fabrication of uniform thin coatings of multi-walled carbon nanotubes (MWCNTs) by electrophoretic deposition (EPD) on semiconductor (silicon) substrates with 3-aminopropyl-triethoxysilane (APTES) surface functionalization has been studied extensively in this report. The gradual deposition and eventual film formation of the carbon nanotubes (CNTs) is greatly assisted by the Coulombic force of at...

Electrophoretic deposition of carbon nanotubes (CNTs) using alternating current electric fields (0.01-1000 Hz) is reported. Pure acetone was used as suspending medium. Two parallel gold electrodes were used as depositing substrate. The effect of depositing parameters such as frequency and three waveforms (sinusoidal, rectangular and triangular) on deposit yield was investigated. According to ou...

Viscosity, electrical conductivity and deposit weight were determined for Electrophoretic deposition (EPD) Mg2+-, Y3+-, La3+- and Ce4+-doped alumina's ethanolic suspensions prepared at dopant concentration between 350 to 1350 ppm. The concentration of XCly (X, y were: Mg, 2; Y, 3; Ce, 3 and La, 3, respectively) the charging salt, is also found to be a critical factor to control the viscosity. I...

The zirconia stabilized by 3mol % Y2O3 (3YSZ) was applied onto the surface of the magnesium alloy AZ91D using electrophoretic deposition (EPD) from a non- aqueous solution. A Ni-P interlayer between the substrate and YSZ coating was also prepared by electroless plating. Finally, coatings were heat treated in control atmosphere at 400 °C. The preparation, microstructure and corrosion resistance ...