نتایج جستجو برای: tensile shear strength

تعداد نتایج: 281131  

There is an increasing need to determine accurately the strength properties of tendons for an effective ground control on mines and underground structures as well as on modelling simulations. The strength properties of cables, used as cable bolts, have been evaluated mainly by their ultimate tensile strength, as this kind of test can be carried out in the field as well as in the laboratory. Onl...

Journal: :Journal of biomechanics 2012
Arnav Sanyal Atul Gupta Harun H Bayraktar Ronald Y Kwon Tony M Keaveny

The shear strength of human trabecular bone may influence overall bone strength under fall loading conditions and failure at bone-implant interfaces. Here, we sought to compare shear and compressive yield strengths of human trabecular bone and elucidate the underlying failure mechanisms. We analyzed 54 specimens (5-mm cubes), all aligned with the main trabecular orientation and spanning four an...

2005
T. Ueda

This paper summarizes a series of studies on the interface of fiber reinforced polymer laminates externally bonded to concrete substrates, carried out in the Laboratory of Engineering for Maintenance Systems, Hokkaido University. Appropriate test methods and bond models for shear bond, tensile bond and cleavage bond (bond under dowel force) are shown. Finally, experimental results on shear bond...

Journal: :Journal of cell science 2011
Phrabha S Raman Christina S Alves Denis Wirtz Konstantinos Konstantopoulos

P-selectin and fibrin(ogen) have pivotal roles in the hematogenous dissemination of tumor cells. CD44 variant isoforms, CD44v, have been identified as the major functional P-selectin ligands and fibrin receptors on metastatic colon carcinoma cells. The molecular recognition of CD44v by fibrin mediates firm adhesion at low shear, whereas CD44v-P-selectin binding supports transient rolling intera...

Journal: :Proceedings of the National Academy of Sciences of the United States of America 2007
Yinmin Wang Ju Li Alex V Hamza Troy W Barbee

It is known that the room-temperature plastic deformation of bulk metallic glasses is compromised by strain softening and shear localization, resulting in near-zero tensile ductility. The incorporation of metallic glasses into engineering materials, therefore, is often accompanied by complete brittleness or an apparent loss of useful tensile ductility. Here we report the observation of an excep...

2013
Wei Lu Yingcheng Hu Jia Yao Yanfang Li

The performance of veneer joints is known to affect the quality of laminated veneer lumber (LVL), so experimental research and simulation analysis of the tensile properties of lap joints were performed and reported in this paper. The lap length, specimen thickness, and specimen width were selected as the experimental factors. The maximum tensile load increased with the increase of each factor; ...

2016
Jong Won Kim Joon Seok Lee

A laminated composite was produced using a thermoplastic prepreg by inserting an interleaved film with the same type of matrix as the prepreg during the lay-up process to improve the low interlaminar properties, which is a known weakness of laminated composites. Carbon fiber fabric (CFF) and polypropylene (PP) were used to manufacture the thermoplastic prepregs. Eight prepregs were used to prod...

2015
Xianqi Lei Congling Li Xinghua Shi Xianghong Xu Yujie Wei

It is generally observed that the existence of geometrical discontinuity like notches in materials will lead to strength weakening, as a resultant of local stress concentration. By comparing the influence of notches to the strength of three typical materials, aluminum alloys with intermediate tensile ductility, metallic glasses with no tensile ductility, and brittle ceramics, we observed streng...

2017
Elham Abu-Alhaija Mohammad Jaradat Ahed Alwahadni

BACKGROUND Molar bonding procedures need continuous improvement to be widely accepted clinically and eventually replace molar bands. MATERIAL AND METHODS The purpose of this study was to determine the effects of enamel micro-abrasion and silane coating of the base of molar tubes on shear and tensile bond strengths of orthodontic molar tubes. A total of 200 third molars were randomly allocated...

2016
R. A. Kellogg Alan M. Russell Thomas A. Lograsso A. B. Flatau A. E. Clark Marilyn Wun-Fogle

Single crystal specimens of Fe-17 at. % Ga were tested in tension at room temperature. Specimens with a tensile axis orientation of [110] displayed slip lines on the specimen faces corresponding to slip on the {110}with a critical resolved shear stress of 220 MPa. Yielding began at 0.3% elongation and 450 MPa. An ultimate tensile strength of 580 MPa was observed with no fracture occurring throu...