نتایج جستجو برای: High carbon steel wire

تعداد نتایج: 2366035  

Journal: :international journal of iron & steel society of iran 2011
s. sadeghpour

the effects of steel wire patenting process parameters on very fine interlamellar spacing in the pearlitic steel wire were investigated and the optimized condition of the process was achieved. in this work, the initial nanopearlitic structure was obtained in a 0.72 wt% carbon steel wire before the wire drawing process. the results were the minimum interlamellar spacing of 35 nm and maximum ulti...

J. M. Prajapati S. S. Patel

Wire electric discharge machine (WEDM) is spark erosion in unconventional machining technique to cut hard and the conductive material with a wire as an electrode. The blanking die material SKD 11 is a high carbon and high chromium tool steel with high hardness and high wearing resistance property. This tool steel has broad application in press tools and dies making industries. In this research ...

The effects of steel wire patenting process parameters on very fine interlamellar spacing in the pearlitic steel wire were investigated and the optimized condition of the process was achieved. In this work, the initial nanopearlitic structure was obtained in a 0.72 wt% carbon steel wire before the wire drawing process. The results were the minimum interlamellar spacing of 35 nm and maximum ulti...

Journal: :Transactions of the Iron and Steel Institute of Japan 1986

2012
J K Singh

Causes for deposition of defective galvanized coating (lumpy deposition of coating during hot dip galvanizing) of carbon-steel wire have been investigated. It is established that the lumpy deposition is caused due to segregation of silicon on the surface of steel wire. Due to this change in composition of the steel at surface, the regions get modified and lie in Sandelin hyper reactive zone. Th...

Journal: :Transactions of the Iron and Steel Institute of Japan 1977

2016
Chih-Cheng Yang Chang-Lun Liu

Cold forging is often applied in the fastener industry. Wires in coil form are used as semi-finished products for the production of billets. This process usually requires preliminarily drawing wire coil in order to reduce the diameter of products. The wire usually has to be annealed to improve its cold formability. The quality of spheroidizing annealed wire affects the forming quality of screws...

2013
W. Sharatchandra Singh B.P.C. Rao B. Sasi S. Vaidyanathan T. Jayakumar Baldev Raj Indira Gandhi

There is an increasing demand for using high sensitive sensors which can detect very low levels of magnetic flux leakage from hidden defects or far-side wall loss due to pitting or local corrosion in ferromagnetic steels. This paper discusses the use of highly sensitive tiny GMR sensors for detection of sub-surface defects in carbon steel plates. Notches located at different depths below surfac...