A. Mahdavian A. Shafyei, D. Haghshenas E. Keshavarz Alamdari

In this Study, vanadium recovery from the steelmaking converter slag was studied. Salt roasting-basic leaching is the process which was applied to separate and extract vanadium from steel making slag. Ground slag was roasted after mixing with determined quantities of sodium carbonate. The effect of time and temperature of roasting and sodium carbonate content were studied. The optimum temperatu...

Journal: :international journal of iron & steel society of iran 2006
a. mahdavian a. shafyei e. keshavarz alamdari d. f. haghshenas

in this study, vanadium recovery from the steelmaking converter slag was studied. salt roasting-basic leaching is the process which was applied to separate and extract vanadium from steel making slag. ground slag was roasted after mixing with determined quantities of sodium carbonate. the effect of time and temperature of roasting and sodium carbonate content were studied. the optimum temperatu...

2011
Oktay Bayat Volkan Arslan Belgin Bayat

Colemanite is one of the most important underground riches of Turkey, having approximately 60% of the world boron deposits, and it has a large portion in the deposits. In this study, chemical leaching and biological leaching methods were used for production of boric acid from colemanite (2CaO · 3B3O3 · 5H2O) (Emet-Kütahya, Turkey). Oxalic acid concentration, temperature, stirring time and solid...

Journal: :Journal of hazardous materials 2005
Chuen-Chang Lin Hong-Long Lin

Soil contamination by heavy metals is increasing. The biosorption process for removal of the heavy metal Cd(2+) from contaminated soil is chosen for this study due to its economy, commercial applications, and because it acts without destroying soil structure. The study is divided into four parts (1) soil leaching: the relationships between the soil leaching effect and agitation rates, solvent c...

2015
Li-Po He Shu-Ying Sun Xing-Fu Song Jian-Guo Yu

This study focused on the leaching process for the recycling of Li, Ni, Co, and Mn from the LiNixCoyMnzO2 (NCM) cathodes of spent lithium-ion batteries (LIBs). Eh–pH diagrams were used to analyze suitable leaching conditions. Operating variables, such as the concentration of H2SO4 (0.5–2.5 M), concentration of H2O2 (0–1 vol%), temperature (10–50 °C), stirring speed (400–800 rpm), and solid/liqu...

2015
Manoj Kumar Jae-chun Lee Min-Seuk Kim Jinki Jeong Kyoungkeun Yoo

This study aims to understand the acid-leaching behavior of metals from 2 to 4 mm waste printed circuit boards (WPCBs) containing 22.0% ± 1.1 Cu, 6.7% ± 0.2 Ca, 0.68% ± 0.02 Sn, 0.59 ± 0.01 % Pb, 2.71% ± 0.08 Al, 0.22% ± 0.01 Fe, etc.. Copper leaching was increased for sulfuric acid concentrations up to 1.2 mol/L and hydrogen peroxide concentrations of 10.0 vol% for a pulp density of 100 g/L at...

Journal: :iranian journal of chemistry and chemical engineering (ijcce) 2004
mahmoud abdollahy seid ziadin shafaei

the recovery process of selenium from iranian sar-cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. the copper anode slimes are made up of those components of  the anodes, which are not soluble in the electrolyte. they contain varying quantities of precious metals like gold, silver, selenium and tellurium. they are being extracted as a by product in the co...

Mahmoud Abdollahy Seid Ziadin Shafaei

The recovery process of selenium from Iranian Sar-Cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. The copper anode slimes are made up of those components of  the anodes, which are not soluble in the electrolyte. They contain varying quantities of precious metals like gold, silver, selenium and tellurium. They are being extracted as a by product in th...

Alafara Abdullahi Baba Daud Temitope Olaoluwa Folahan Amoo Adekola Musa John Saliu Rafiu Babatunde Bale Taofiqat Omotayo Abu

This study investigated the optimum conditions for the leaching of manganese-rich iron ore for subsequent beneficiation studies in laboratory scale. The experiments were carried out by varying the concentration of H2 SO4 solution and the leaching temperature. The properties of the iron ore was characterized by X-ray fluorescence (XRF), X-ray diffraction (XRD), Scanning Electron Microscopy (SEM)...

Journal: :journal of mining and environment 2016
mohammad rezaee rad shahrokh shahhoseini mehdi janfada hosein ali mirzaee parviz kelidari

low grade diasporic bauxite in the jajarm mine with an a/s (al2o3/sio2) ratio of 2.3 is not usable in the bayer process at jajarm alumina complex. due to the severe interlocking effect between the diaspore and aluminosilicate minerals (chamosite and kaolinite) and iron-containing minerals in a microcrystal matrix, the thermo-chemical treatment, which is independent from micro-mineralogy, was ch...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید