نتایج جستجو برای: hard porcelain
تعداد نتایج: 149771 فیلتر نتایج به سال:
It has been demonstrated that a Cs(2)O-stabilized leucite porcelain was susceptible to a stress-induced phase transformation, but toughening was not observed.1 It was hypothesized that if Cs(2)O-stabilized leucite core particles were added to a cesium-free matrix porcelain, selected or designed to enhance the toughening mechanism, toughening would occur. A commercial porcelain (VP) and a synthe...
Introduction 'Porcelain aorta' is listed in the second consensus document of the Valve Academic Research Consortium as a risk factor in aortic valve replacement. However, the extent of circumferential involvement is poorly defined with great variability in reported incidence. We present a simple, reproducible classification to describe the extent of aortic calcification and thus appropriately d...
Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cy...
The wear performances of bovine tooth enamel (BTE) against translucent tetragonal zirconia polycrystals (TZP) compared to that of feldspar porcelain and the influence of surface treatments of translucent TZP were investigated by the two-body wear test. Translucent TZP and feldspar porcelain were used as hemisphere abrader specimens with a radius of curvature of 5 mm; flat BTE surfaces were used...
This paper presents the effect of selected parameters of abrasive blasting on the strength of a joint between dental porcelain and metal base. Experiments were conducted for different grain sizes of abrasive material and different blasting angles, with a constant blasting pressure. InLine dental porcelain was fused on samples of cobalt-chromium alloy following abrasive blasting; they were subse...
PURPOSE The purpose of this study was to compare microshear bond strength of three different luting resins using a new microshear method closely simulating clinical condition. METHODS Thirty 1-mm-thick slices of intact human first molars and thirty 0.8-mm-diameter feldspathic porcelain rods were etched by 37% phosphoric acid for enamels and 9.5% hydrofluoric acid for porcelains. Adhesive (Mar...
STATEMENT OF PROBLEM Ceramic restorations should be made of porcelain layers of different opacity, shade, and thickness in order to provide a natural appearance. By means of CAD/CAM layering technology such as CICERO, it is feasible to produce all-ceramic crowns with porcelain layers of predetermined thickness. However, it is not yet known whether changes in thickness of these porcelain layers ...
AIM To achieve acceptable contour, color, esthetics, and occlusal relations, the porcelain may be subjected to several firing cycles. This study sought to assess the effect of multiple firing cycles on the microtensile bond strength (MTBS) of lithium disilicate-based ceramics (e.max Press, e.max CAD). MATERIALS AND METHODS IPS e.max computer aided design (CAD) cores were fabricated using CAD/...
BACKGROUND With the emergence of a completed genome sequence of the freshwater crustacean Daphnia pulex, construction of genomic-scale sequence databases for additional crustacean sequences are important for comparative genomics and annotation. Porcelain crabs, genus Petrolisthes, have been powerful crustacean models for environmental and evolutionary physiology with respect to thermal adaptati...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید