A discrete dislocation dynamics study of precipitate bypass mechanisms in nickel-based superalloys

نویسندگان

چکیده

Order strengthening in nickel-based superalloys is associated with the extra stress required for dislocations to bypass $\gamma'$ precipitates distributed $\gamma$ matrix. A rich variety of mechanism has been identified, various shearing and Orowan looping processes giving way climb as operating conditions change from low/intermediate temperatures high regime, temperature low regime. When anti phase boundary (APB) mechanisms operate, changes increased particle size within a broad coexistence window. Another possibility, supported by indirect experimental evidence, that third "hybrid" transition may operate. In this paper we use discrete dislocation dynamics (DDD) simulations study Ni-based superalloys. We develop new method compute generalized stacking fault forces DDD simulations. square lattice spherical $a/2\langle110\rangle\{111\}$ edge dislocations, function volume fraction size. show hybrid possible it operates between regimes over large range radii. also consider effects $\gamma/\gamma'$ misfit on mechanisms, which approximate an additional precipitate computed according Eshelby's inclusion theory. looping-shearing regimes, generally results stress. For sufficiently misfit, controlled pinning trailing exit side precipitates.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Dislocation-precipitate Interaction in Discrete Dislocation Dynamics

This contribution deals with the numerical simulation of dislocation dynamics by means of parametric mean curvature flow. Dislocations are described as an evolving family of closed and open smooth curves driven by the normal velocity. The equation is solved using direct approach by semi-discrete scheme based on finite difference method. Numerical stability is improved by tangential redistributi...

متن کامل

the study of bright and surface discrete cavity solitons dynamics in saturable nonlinear media

امروزه سالیتون ها بعنوان امواج جایگزیده ای که تحت شرایط خاص بدون تغییر شکل در محیط منتشر می-شوند، زمینه مطالعات گسترده ای در حوزه اپتیک غیرخطی هستند. در این راستا توجه به پدیده پراش گسسته، که بعنوان عامل پهن شدگی باریکه نوری در آرایه ای از موجبرهای جفت شده، ظاهر می گردد، ضروری است، زیرا سالیتون های گسسته از خنثی شدن پراش گسسته در این سیستم ها بوسیله عوامل غیرخطی بوجود می آیند. گسستگی سیستم عامل...

Modelling plastic deformation in a single-crystal nickel-based superalloy using discrete dislocation dynamics

Background: Nickel-based superalloys are usually exposed to high static or cyclic loads in non-ambient environment, so a reliable prediction of their mechanical properties, especially plastic deformation, at elevated temperature is essential for improved damage-tolerance assessment of components. Methods: In this paper, plastic deformation in a single-crystal nickel-based superalloy CMSX4 at el...

متن کامل

Diffusion Welding of Nickel-based Superalloys

Ni based superalloys can be welded by diffusion bonding. Temperature, diffusion coefficient, activation energy and Boltzmann constant influence the quality of diffusion bonding, so obtaining the best condition for welding is considered. Showing the suitable condition for diffusion welding of nickel-based superalloys is the aim of this paper.

متن کامل

Dislocation dynamics in nanocrystalline nickel.

It is believed that the dynamics of dislocation processes during the deformation of nanocrystalline materials can only be visualized by computational simulations. Here we demonstrate that observations of dislocation processes during the deformation of nanocrystalline Ni with grain sizes as small as 10 nm can be achieved by using a combination of in situ tensile straining and high-resolution tra...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: International Journal of Plasticity

سال: 2021

ISSN: ['1879-2154', '0749-6419']

DOI: https://doi.org/10.1016/j.ijplas.2021.103062