Analysis of Connecting Rod Fatigue Fracture Surface by X-Ray Fractography.
                    
                        
                            نویسندگان
                            
                            
                        
                        
                    
                    
                    چکیده
منابع مشابه
Surface Hardness Measurment and Microstructural Characterisation of Steel by X-Ray Diffraction Profile Analysis
An X-ray diffraction line will broaden considerably when steels change into martensitic structure on quenching. The results presented in this paper show that X-ray diffraction technique can be employed for a rapid and nondestructive measurement of hardness of hardened steel. Measurement on various quenched and tempered steels showed that the breadth of its diffraction peak increased with increa...
متن کاملStudy and Simulation of Shot peening Effect on Fatigue Life of a Powder Forged Connecting rod
Shot peening applies a residual compressive stress field (RCSF) on the surface of parts. It also shifts “crack nucleation sites” to sub-surface locations. A nondestructive method of measuring the stresses, Sin2ψ was utilized here and the stress values introduced to Ansys software. For this purpose, uniform stress in all directions was applied on the con rod. Loading on the rod in Ansys had thre...
متن کاملStudy of the Fatigue Fracture Surface Regions of Steels Using Microbeam Synchrotron X-Ray Diffraction
A cyclic plastic zone area near fatigue-fractured surface was studied using a back-reflection camera and high intensity, microbeam, synchrotron X-ray source (SR) in order to measure the variation of the stress intensity factor range (AK) along the fatigue fracture. The existence of subgrains within the cyclic plastic region was shown by the appearance of small spots in the Debye-Scgerrer rings ...
متن کاملMetamodel-based Shape Optimization of Connecting Rod Considering Fatigue Life
To optimize a connecting rod satisfying fatigue life, metamodel-based design optimization is proposed. To approximately predict both volume and fatigue life of connecting rod, kriging metamodel is constructed based on maximin eigenvalue sampling. Fatigue analysis is accomplished for the calculation of fatigue life. The results of metamodel-based design optimization are compared with those of cl...
متن کاملStress and Fatigue of Connecting Rod in Light Vehicle Engine
The connecting rod (CR) is the main moving parts and an important component of engine. If the reliability is not strong enough, fatigue failure of the CR would occur, thereby leading to component fracture and engine failure. So much so that CR fracture. It will lead to engine fault as well as serious outcome. In this paper, stress distribution and fatigue life of CR in light vehicle engine were...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Society of Materials Science, Japan
سال: 2000
ISSN: 1880-7488,0514-5163
DOI: 10.2472/jsms.49.1143