Fractographic Study on Sulfide Cracking of Mild Steel
نویسندگان
چکیده
منابع مشابه
Sulfide Stress Cracking Behavior of a Martensitic Steel Controlled by Tempering Temperature
A medium-carbon Cr-Mo-V martensitic steel was thermally processed by quenching (Q) at 890 °C and tempering (T) at increasing temperatures from 650 °C to 720 °C and the effect of tempering temperature, Tt, on sulfide stress cracking (SSC) behaviors was estimated mainly via double cantilever beam (DCB) and electrochemical hydrogen permeation (EHP) tests and microstructure characterization. The re...
متن کاملFractographic Investigation of Failure in Stainless Steel Orthopedic Plates
Plates of austenitic stainless steel are often used in orthopedic surgery for fixing ends of the broken bones and for repairing fractures. The paper analyzes a premature breakage of six plates for fixing broken bones with different patients during their recovery. Each plate's breakage can induce serious aftermaths such as a new surgery, unexpected undesired complications and a prolonged healing...
متن کاملA mortality study among mild steel and stainless steel welders.
A mortality study was carried out in conjunction with the European mortality study among welders coordinated by the International Agency for Research on Cancer (IARC). The study was aimed at assessing risks for lung cancer in relation to exposure to asbestos, welding fumes containing chromium and nickel, and tobacco smoke. The study included a cohort of 2721 welders and an internal comparison g...
متن کاملa study on construction of iranian life tables: the case study of modified brass logit system
چکیده ندارد.
15 صفحه اولEffect of Nonmetallic Inclusions on Steel Welds Metal Hot Cracking
B. Z orc, W elding I nstitute, L jubljana, S lovenia; M . I mamović, Un iversity of Zenica, Faculty of Mechanical Engineering, Zenica, B a nd H; A. Nagode, B. Kosec, L. Kosec, University of Ljubljana, Faculty of Natural Sciences and Engineering, Ljubljana, Slovenia; A. Stoić, I. Samardžić, University of Osijek, Mechanical Engineering Faculty, Slavonski Brod, Croatia Intercrystally distributed n...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Institute of Metals and Materials
سال: 1974
ISSN: 0021-4876,1880-6880
DOI: 10.2320/jinstmet1952.38.3_254