Fractography of CTOD Specimens in Welded Joints of 21/4Cr-1Mo Steel

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Study on Microstructure and Mechanical Properties of Laser Welded Joints of 1.7225 Steel

The aim of the present study is to investigate the mechanical and microstructural properties of 1.7225 steel in laser welding process using Nd:YAG pulsed laser device and then to determine the optimal focal length relative to the part in the welding area. After welding, microstructural characterization, microhardness and tensile tests were performed. Evaluations showed that the optimal focal le...

متن کامل

Study on Microstructure and Mechanical Properties of Laser Welded Joints of 1.7225 Steel

The aim of the present study is to investigate the mechanical and microstructural properties of 1.7225 steel in laser welding process using Nd:YAG pulsed laser device and then to determine the optimal focal length relative to the part in the welding area. After welding, microstructural characterization, microhardness and tensile tests were performed. Evaluations showed that the optimal focal le...

متن کامل

The Influence of Ultrasonic Impact Treatment on Fatigue Behaviour of Welded Joints in High-strength Steel

The unabated growth of the steel industry and progressively increasing operating loads on metal structures generate a need for a search for optimum engineering solutions to improve the loadcarrying capacity and reduce metal consumption. One way of resolving this problem is to utilise high-strength steels. It is common knowledge however that the improvement of the steel strength is accompanied b...

متن کامل

Effect of Welding Parameters in the Microstructure and Mechanical Properties of Friction-Welded Joints of 100Cr6 Steel

 In this study, high-carbon, chromium alloy steel (100Cr6) having the initial spheroidized microstructure was welded using the rotary friction welding method. The effects of process parameters such as friction time and friction force were experimentally investigated. The friction welded joints were produced of two 100Cr6 steel rods. In order to examine the microstructure and mechanical properti...

متن کامل

Fatigue Life of Repaired Welded Tubular Joints

In this study, the effect of repair on fatigue life of tubular joints is investigated. Six cracked specimens precedently subjected to fatigue loading undergone to weld repair. Two of those specimens were shot peened before primary fatigue loading.  It is shown that repair gives rise to about 150% increase in fatigue life for original specimens while the increase of fatigue life for shot-peened ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Microscopy and Microanalysis

سال: 2003

ISSN: 1431-9276,1435-8115

DOI: 10.1017/s1431927603443535