High-Entropy Brazing Filler Metal Based on NiCoCrPdGe System for Brazing Nickel Superalloys

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Vacuum Brazing of Zirconium-Based Alloy and 321 Stainless Steel Using Titanium Based Filler Metal

Both Zirconium-based alloys and 321stainless steel are widely used as engineering alloys due to their good mechanical properties. Conventional fusion welding techniques for Zr alloys and stainless steel are not feasible due to the formation of brittle intermetallic compounds such as (Zr3Fe, ZrFe2 and Zr2Fe) and corrosion cracking. Brazing is one of the most wide...

متن کامل

Wettability of Brazing Filler Metals on Copper and Copper Alloys

The possibility of alloying can not be avoided at the interface between molten brazing filler metal and base metal in brazing, so the wettability of brazing filler metal can not be easily explained theoretically. We used the original apparatus for wettability test and investigated the relation between the wettability of brazing filler metals of Ag-P-Cu and Ag-Cu-Zn-Cd systems on copper and the ...

متن کامل

Investigation on effect of holding time in brazing of steel to cemented carbide using Cu-Ag alloy filler metal

Nowadays, cemented carbides-steels joints by brazing method are taken into consideration. One of the problems of these joints is the creation residual stresses that can reduce it with choose correct parameters of brazing. In this study, Silver base alloy filler containing copper, zinc and cadmium have been used in temperature 780°C and the effect of time parameter 5, 10 and 15 minutes on micros...

متن کامل

Brazing & Soldering Today

Brazed components play an essential role in consistent joining techniques. The brazing process is characterized by low process temperatures and fast processing times, compared to welding techniques. Beside the resulting low manufacturing costs, brazing can join dissimilar materials, e.g. metals and ceramics. Consequently, brazing provides potential for many industrial applications like the prod...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallofizika I Noveishie Tekhnologii

سال: 2023

ISSN: ['1024-1809', '2617-1511']

DOI: https://doi.org/10.15407/mfint.45.03.0387