Initiation and Propagation Processes of Internal Fatigue Cracks in β Titanium Alloy Based on Fractographic Analysis

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A Study of Fatigue Crack Initiation in a Two Phase Β-metastable Titanium Alloy

α/β titanium alloys are choice materials for aeronautical and automotive industries due to their high performance to density ratio. For several applications, fatigue resistance is one of the critical design parameter. Particularly, initiation of fatigue crack plays a key role. Furthermore, hardly anything can be found in the literature on the fatigue crack initiation in multiphase microstructur...

متن کامل

Fatigue and corrosion fatigue properties of Ti-6Al-4V implant grade titanium alloy in Ringer solution

Nowadays modification of metallic biomaterials which are used as implants for bone and hard tissues replacement is considered as an important subject. In the current study, corrosion fatigue properties of Ti-6Al-4V alloy investigated via Rotating-Bending standard test method and then, the results compared with the fatigue properties of the specimens tested in the same conditions. Scanning elect...

متن کامل

Initiation of fatigue cracks in AZ91 Mg alloy processed by ECAP

Mechanism of fatigue crack initiation was investigated in ultrafine-grained (UFG) magnesium alloy AZ91 processed by equal channel angular pressing (ECAP). Fatigue behaviour of UFG material was compared to the behaviour of material in an initial as-cast state. Focused ion beam technique (FIB) was applied to reveal the surface relief and early fatigue cracks. Two substantially different mechanism...

متن کامل

The Growth of Small Corrosion Fatigue Cracks in Alloy

The corrosion fatigue crack growth characteristics of small (>35pm) surface and corner cracks in aluminum alloy 7075 is established. The early stage of crack growth is studied by performing in situ long focal length microscope (500X) crack length measurements in laboratory air and 1% NaCl environments. To quantify the “small crack effect” in the corrosive environment, the corrosion fatigue crac...

متن کامل

Dynamic Initiation and Propagation of Multiple Cracks in Brittle Materials

Brittle materials such as rock and ceramic usually exhibit apparent increases of strength and toughness when subjected to dynamic loading. The reasons for this phenomenon are not yet well understood, although a number of hypotheses have been proposed. Based on dynamic fracture mechanics, the present work offers an alternate insight into the dynamic behaviors of brittle materials. Firstly, a sin...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Sciences

سال: 2020

ISSN: 2076-3417

DOI: 10.3390/app11010131