Long term microstructural stability of intermetallic Ti-46Al-8Ta alloy during ageing at temperatures of 700-800 °C

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The phase evolution, mechanical behavior, and microstructural instability of a fully-lamellar Ti–46Al(at.%) alloy

A Ti–46Al(at.%) polysynthetically twinned alloy, which contained a characteristic lamellar spacing of k 1⁄4 1:3 lm, was converted to a polycrystalline fully-lamellar microstructure with k 1⁄4 19:9 nm using an a-phase solution treatment followed by a2 þ c aging. Tensile experiments, performed on microsamples extracted from within single grains of the polycrystalline material, illustrated that ul...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

Microstructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation

Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...

متن کامل

Application of T-shape Friction T test for Ti-6Al-4V Alloy at Elevated Temperatures

There are several parameters that have significant influence in metal forming process. One of the most important of them is friction coefficient. Friction can change the pattern of metal flow and the force needed for deformation. It is necessary to determine the friction coefficient to study the effect of friction on metal forming process. This study is concerned with numerical and experimental...

متن کامل

intermetallic phase formation during combustion synthesis of mechanically activated ni-ti alloy

intermetallic phase formation and oxidation reaction during combustion synthesis (cs) of ni-ti equiatomic mixture are affected by mechanical activation (ma) and pre-heating conditions. important parameters are ignition time, reaction duration, temperature rise, microstructural change, titanium oxidation and intermetallic phase formation. superelasticity and shape memory effects are influenced b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallic Materials

سال: 2010

ISSN: 0023-432X