Microstructure and defects in a Ni-Cr-Al-Ti γ/γ’ model superalloy processed by laser powder bed fusion

نویسندگان

چکیده

Additive manufacturing (AM) of non-weldable high-γ’ Ni base superalloys is challenging due to various issues, but notably because their inherent cracking propensity. Typically, the segregation melting point-depressant elements grain boundaries (GB) drastically increases solidification interval, allowing high processing-induced stresses in parts pull apart liquid film at GBs. To achieve a better understanding consolidation process nickel as well origin defects and cracks, simplified model γ/γ’-strengthened Ni-Cr-Al-Ti alloy with reduced related commercial CM247LC alloy, investigated under large parameter survey. The behavior typical produced by AM, optimal condition being compromise between porosity. mechanism is, however, changed solid-state cracking, localized high-angle GBs, likely lack GB strengthening phases inherently low strength this alloy. Transmission electron microscopy atom probe tomography reveal elemental Ti, lower extent Cr Al, cell boundaries, agreement Calphad calculations. No γ’ precipitates are observed as-processed condition, indicating that all remain solid solution. chemical differences cracked non-cracked boundaries. Trace amounts oxygen contained powder lead Al2O3 slag formation, nano oxide dispersoid incorporation. Sulfur, critical contaminant superalloys, detected rendered harmless formation TiS nanoprecipitates.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Creep of Ni-Al and Ni-Cr-Al Superalloy Foams

The steady-state creep rate of Ni-base metallic foams, with superalloy composition (in wt. pct) Ni7.8∼9.1Al (relative density, ρ = 2.5-2.6) and Ni-13.5∼16.6Cr-5.1∼8.9Al (ρ = 2.8∼3.0), was measured under a range of temperatures (680∼825°C) and applied stresses (0.1∼0.3 MPa), and compared with that of NiAl intermetallic foams (ρ = 5.3). The stress exponent and activation energy are within the exp...

متن کامل

Synthesis, structure, and mechanical properties of Ni–Al and Ni–Cr–Al superalloy foams

Reticulated nickel foams were alloyed with 8–9 wt% Al or 14–18 wt% Cr and 5–9 wt% Al in a three-step method consisting of (i) gas-phase deposition of Cr and/or Al onto the struts of a pure Ni foam by pack-cementation at 1000 C; (ii) homogenization at 1200 C to remove concentration gradients and to solutionize the alloyed struts; (iii) aging at 900 C to form c0 precipitates within the struts. Th...

متن کامل

Nanoscale Cellular Structures at Phase Boundaries of Ni-Cr-Al-Ti and Ni-Cr-Mo-Al-Ti Superalloys

The microstructural evolution of Ni-20 pct Cr wires was studied during pack cementation where Al and Ti, with and without prior cementation with Mo, are deposited to the surface of the NiCr wires and subsequently homogenized in their volumes. Mo deposition promotes the formation of Kirkendall pores and subsequent co-deposition of Al and Ti creates a triple-layered diffusional coating on the wir...

متن کامل

Study of the Microstructure and Cracking Mechanisms of Hastelloy X Produced by Laser Powder Bed Fusion

Hastelloy X (HX) is a Ni-based superalloy which suffers from high crack susceptibility during the laser powder bed fusion (LPBF) process. In this work, the microstructure of as-built HX samples was rigorously investigated to understand the main mechanisms leading to crack formation. The microstructural features of as-built HX samples consisted of very fine dendrite architectures with dimensions...

متن کامل

Laser powder bed fusion of Ti-6Al-4V parts: Thermal modeling and mechanical implications

A continuum-scale modeling approach is developed and employed with three-dimensional finite element analysis (FEA), for simulating the temperature response of a Ti-6Al-4V, two-layered parallelepiped with dimensions of 10×5×0.06 mm during Laser Powder Bed Fusion (L-PBF), a metals additive manufacturing (AM) method. The model has been validated using experimental melt pool measurements from the l...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید