Microstructure correlation in high-strength steels with continuous stiffness mode nanoindentation results. High-resolution vs. low-resolution nanoindentation

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

High-Strength Bainitic Steels

With careful design, mixed microstructures consisting of fine plates of upper bainitic ferrite separated by thin films of stable retained austenite have exhibited impressive combinations of strength and toughness in highsilicon bainitic steels. The silicon suppresses the precipitation of brittle cementite leading to an improvement in toughness. The essential principles governing the optimisatio...

متن کامل

Nanoindentation and contact-mode imaging at high temperatures

Technical issues surrounding the use of nanoindentation at elevated temperatures are discussed, including heat management, thermal equilibration, instrumental drift, and temperature-induced changes to the shape and properties of the indenter tip. After characterizing and managing these complexities, quantitative mechanical property measurements are performed on a specimen of standard fused sili...

متن کامل

Nanoindentation of wood cell walls: Continuous stiffness and hardness measurements

The objective of this study was to measure the mechanical properties of individual, native wood fibers using the continuous nanoindentation measurement technique. The indentation depth profile exhibited a small length-scale effect, which was confirmed using the size-effect index derived from the indentation loading curve. The hardness (Hu) or stiffness (Eu) values determined from indentation un...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

Ultra High Strain Rate Nanoindentation Testing

Strain rate dependence of indentation hardness has been widely used to study time-dependent plasticity. However, the currently available techniques limit the range of strain rates that can be achieved during indentation testing. Recent advances in electronics have enabled nanomechanical measurements with very low noise levels (sub nanometer) at fast time constants (20 µs) and high data acquisit...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Mechanical Behaviour of Materials

سال: 2013

ISSN: 2191-0243,0334-8938

DOI: 10.1515/jmbm-2013-0004