Microstructure Evolution of Ni-base Superalloy 625: from Conventional Thermomechanical Processed to Selective Laser Melting Processed

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

Mechanical Properties of Pure Titanium Models Processed by Selective Laser Melting

The influence of laser processing parameters on mechanical properties and microstructure of pure titanium models made by selective laser melting is investigated. The density of the models can reach higher than 95% under proper conditions. Although the tensile strength test shows results comparable to the wrought material, the impact and torsional fatigue strengths are low because of porosity an...

متن کامل

Microstructure evolution and mechanical properties of Mo40/C93200 bimetal processed by compound casting process

Compound casting refers to a process that used to produce bimetals. This study investigates the interface of Mo40/C93200 that is produced by compound casting process. In this research, molten bronze is poured around steel core, interaction between liquid and solid creates a diffusion zone and followed by a transition layer which leads to the creation of diffused region between the interfaces of...

متن کامل

Microstructure and Mechanical Properties of Inconel 625 and 7 18 Alloys Processed by Powder Injection Molding

Powder injection molding of superalloys offer a potential route for the manufacture of small and geometrically complex components for the aircraft engine industry. In this investigation, 625 and 718 alloy powders with an average size below 10 pm were injection molded into tensile test bars which were then sintered in a hydrogen atmosphere at diverse temperatures after debinding. Other 718 alloy...

متن کامل

A synchrotron study of microstructure gradient in laser additively formed epitaxial Ni-based superalloy

Laser additive forming is considered to be one of the promising techniques to repair single crystal Ni-based superalloy parts to extend their life and reduce the cost. Preservation of the single crystalline nature and prevention of thermal mechanical failure are two of the most essential issues for the application of this technique. Here we employ synchrotron X-ray microdiffraction to evaluate ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Microscopy and Microanalysis

سال: 2017

ISSN: 1431-9276,1435-8115

DOI: 10.1017/s1431927617011916