Nanoindentation behaviour of layered silicate filled spent polyamide-12 nanocomposites
                    
                        
                            نویسندگان
                            
                            
                        
                        
                    
                    
                    چکیده
منابع مشابه
Polymer Layered Silicate Nanocomposites: A Review
This review aims to present recent advances in the synthesis and structure characterization as well as the properties of polymer layered silicate nanocomposites. The advent of polymer layered silicate nanocomposites has revolutionized research into polymer composite materials. Nanocomposites are organic-inorganic hybrid materials in which at least one dimension of the filler is less than 100 nm...
متن کاملPolymer- Layered Silicate Nanocomposites for Cryotank Applications
Previous composite cryotank designs have relied on the use of conventional composite materials to reduce microcracking and permeability. However, revolutionary advances in nanotechnology derived materials may enable the production of ultra-lightweight cryotanks with significantly enhanced durability and damage tolerance, as well as reduced propellant permeability. Layered silicate nanocomposite...
متن کاملPolymer-Layered Silicate Nanocomposites: Synthesis, Properties and Applications
Polymer nanocomposites, especially polymerlayered silicate (PLS) nanocomposites, represent a radical alternative to conventionally (macroscopically) filled polymers. Because of their nanometer-size dispersion, the nanocomposites exhibit markedly improved properties when compared with the pure polymers or conventional composites. These include increased modulus and strength, decreased gas permea...
متن کاملPolymer/layered silicate nanocomposites: a review from preparation to processing
A review is given of the academic and industrial aspects of the preparation, characterization, materials properties, crystallization behavior, melt rheology, and processing of polymer/layered silicate nanocomposites. These materials are attracting considerable interest in polymer science research. Hectorite and montmorillonite are among the most commonly used smectite-type layered silicates for...
متن کاملStudy on the Optical and Rheological properties of polymer- layered Silicate Nanocomposites
This review reports recent advances in the field of polymer–layered silicate nano composites. Thesematerials have attracted both academic and industrial attention because they exhibit dramaticimprovement in properties at very low filler contents. Herein, the structure, preparation andproperties of polymer–layered silicate nanocomposites are discussed in general, and finally the effectof clay na...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Polymer Testing
سال: 2011
ISSN: 0142-9418
DOI: 10.1016/j.polymertesting.2011.05.008