Nanoindentation responses near single grain boundaries in oxide ceramics

نویسندگان

چکیده

Local mechanical responses near single grain boundaries (GBs) of 9.8 mol% Y2O3-stabilized ZrO2 bicrystals, SrTiO3 bicrystal, and Al2O3 polycrystal were investigated by nanoindentation at room temperature to reveal GB contributions the properties. Contrary concept Hall–Petch strengthening, hardness showed negligible variations among interiors, vicinities, just on GBs in samples. Importantly, may be underestimated owing grooving thermally etched Despite change intrinsic hardness, transmission electron microscopy observation specimen under impressions revealed dislocation pileups GBs. These results suggest that oxide ceramics prevented movement but with limited strengthening contributions. This should correspond macroscopic behaviors ceramics, where coefficients normalized friction stress are significantly smaller than those metals.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Grain boundary segregation in oxide ceramics

D PR O Abstract The factors which control grain boundary segregation in oxide ceramics are reviewed. These include grain boundary energy, cation–cation interactions, impurity cation size, as well as electrostatic interactions with the grain boundary space charge. In addition, an approach for measuring grain boundary segregation in those materials, as a function of the five macroscopic parameter...

متن کامل

Nanoindentation Induced Deformation Near Grain Boundaries of Corrosion Resistant Nickel Alloys Citation

The damage accumulation behavior of different grain boundary structures in Inconel 690 (Ni-29wt%Cr-9wt%Fe) was investigated in the presence of large, localized plastic strains induced by nanoindentation. Spatially-resolved hardness was measured as a function of lateral distance from ‘random’ high-angle grain boundaries and twin boundaries. The confinement of induced defects between the indenter...

متن کامل

Dislocations and Grain Boundaries in Ceramics and Metals

This paper is offered as a tribute to the late Gareth Thomas and the celebration of his career using transmission electron microscopy. His early work on dislocations and twin boundaries in metals suggested indirect methods for determining the stacking-fault energies (SFEs) of Al [1] and Ni [2] and subsequently examined questions on how the measured values of SFEs of copper alloys change when th...

متن کامل

Molecular dynamics simulations of nanoindentation and scratch in Cu grain boundaries

The dynamic nanomechanical characteristics of Cu films with different grain boundaries under nanoindentation and scratch conditions were studied by molecular dynamics (MD) simulations. The type of grain boundary is the main factor in the control of the substrate atoms with respect to the size of dislocations since the existence of the grain boundary itself restricts the movement associated with...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the American Ceramic Society

سال: 2022

ISSN: ['0002-7820', '1551-2916']

DOI: https://doi.org/10.1111/jace.18887