Numerical Simulation of Surface Modification During Machining of Nickel-based Superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Parametric optimization of powder mixed electrical discharge machining for nickel-based superalloy inconel-800 using response surface methodology

Background: Electrical Discharge Machining (EDM) is a well-established non-conventional machining process for the machining of electrically conductive and difficult-to-machine materials. But its applications are limited because of the slow machining rate and poor surface finish. Powder mixed EDM (PMEDM) is unitary of the recent progresses in the EDM process in which powder particles mixed in th...

متن کامل

fabrication of new ion sensitive field effect transistors (isfet) based on modification of junction-fet for analysis of hydronium, potassium and hydrazinium ions

a novel and ultra low cost isfet electrode and measurement system was designed for isfet application and detection of hydronium, hydrazinium and potassium ions. also, a measuring setup containing appropriate circuits, suitable analyzer (advantech board), de noise reduction elements, cooling system and pc was used for controlling the isfet electrode and various characteristic measurements. the t...

Constitutive Model Based on Dynamic Recrystallization Behavior during Thermal Deformation of a Nickel-Based Superalloy

Peng Zhang 1, Cen Yi 1, Gang Chen 1, Heyong Qin 2 and Chuanjie Wang 1,* 1 School of Materials Science and Engineering, Harbin Institute of Technology at Weihai, Weihai 264209, China; [email protected] (P.Z.); [email protected] (C.Y.); [email protected] (G.C.) 2 Central Iron & Steel Research Institute, Beijing 100081, China; [email protected] * Correspondence: [email protected]; Tel.: +86-631-568...

متن کامل

Numerical Simulation Of Heat Affected Zone Microstructure During Laser Surface Melting

Microstructural changes during laser welding and laser surface treatment has been regarded by many researchers. Most researches have focused on studying the effect of various process parameters on the size and microstructure of the heat affected zone. But some studies show that the initial microstructure of the base metal can also affect the heat affected zone dimensions and final microstructur...

متن کامل

Laser Cladding of Ultra-Thin Nickel-Based Superalloy Sheets

Laser cladding is a well-established process to apply coatings on metals. However, on substrates considerably thinner than 1 mm it is only rarely described in the literature. In this work 200 µm thin sheets of nickel-based superalloy 718 are coated with a powder of a cobalt-based alloy, Co-28Cr-9W-1.5Si, by laser cladding. The process window is very narrow, therefore, a precisely controlled Yb ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia CIRP

سال: 2015

ISSN: 2212-8271

DOI: 10.1016/j.procir.2015.03.053