Peculiarities of corrosion-mechanical fracture 09G2S pipe steel samples in the conditions cathodic protection were investigated. It was established that depending on level protective potential, stress-corrosion cracking a ferrite-pearlite class can occur by different mechanisms. The range potentials determined, at which anodic dissolution and hydrogen embrittlement simultaneously during steel, namely from -0.85 V to -1.0 V. existence above mechanisms is confirmed change strength viscosity properties morphology fractures. For steels other manufacturing technology grades, these potential areas may differ.
منابع مشابه
An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution
The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...
متن کاملThe Role of Cathodic Poisons on the Stress Corrosion Cracking of Zircaloy- 2 in Methanolic Solution Containing 0.4vol.% Hydrochloric Acid
متن کامل
A Continuum Damage Model for the Stress Corrosion Cracking of Austenitic Stainless Steel
In the present work, the mechanical behavior of stress corrosion cracking phenomenon is described. Such phenomenon presents strong complexity due to metallurgic and electrochemical aspects. A methodology for modeling both SSR (Slow Strain Rate) and CL (Constant Load) tests based upon thermodynamics of continuum solids and elastoplastic damage is proposed. In this macroscopic approach, besides t...
متن کاملTransgranular Stress Corrosion Cracking of 304L Stainless Steel Pipe Clamps in Direct Use Geothermal Water Heating Applications
Direct use geothermal heating relies on heat extracted from naturally occurring geothermal water sources to provide heating needs for commercial and residential use. The city of Boise, Idaho maintains the largest district geothermal heating system in the United States, utilizing a source of geothermal water at 80°C. 304 Stainless steel (UNS S30400) pipe clamps are used throughout the system as ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: ?????? ? ????? ???????? ????
سال: 2021
ISSN: ['1729-4428', '2309-8589']
DOI: https://doi.org/10.15330/pcss.22.4.828-836