Repetitive Ultra-low Stress Induced Nanocrystallization in Amorphous Cu‒Zr‒Al Alloy Evidenced byin situNanoindentation

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Nanocrystallization in Co67Cr7Fe4Si8B14 Amorphous Alloy Ribbons

The nanocrystallization of Co67Fe4Cr7Si8B14 amorphous ribbons which prepared by planar flow melt spinning process (PFMS) was investigated. Crystallization of the ribbons was studied by differential thermal analysis (DTA), X-ray diffraction (XRD) and transmission electron microscopy (TEM). The DTA result of amorphous ribbon at heating rate of 10˚C/min showedoccurrence of phase transitions in two...

متن کامل

nanocrystallization in co67cr7fe4si8b14 amorphous alloy ribbons

the nanocrystallization of co67fe4cr7si8b14 amorphous ribbons which prepared by planar flow melt spinning process (pfms) was investigated. crystallization of the ribbons was studied by differential thermal analysis (dta), x-ray diffraction (xrd) and transmission electron microscopy (tem). the dta result of amorphous ribbon at heating rate of 10˚c/min showedoccurrence of phase transitions in two...

متن کامل

KINETICS OF -Fe NANOCRYSTALLIZATION IN Fe55Cr18Mo7B16C4 BULK AMORPHOUS ALLOY

Abstract: In this research work, crystallization kinetics of Fe55Cr18Mo7B16C4 alloy was evaluated by X-ray diffraction, TEM observations and differential scanning calorimetric tests. In practice, crystallization and growth mechanisms were investigated using DSC tests in four different heating rates. Results showed that a two -step crystallization process occurred in the alloy in which - Fe phas...

متن کامل

NANOCRYSTALLIZATION MECHANISMS OF Fe52Cr18Mo7B16C4Nb3 BULK AMORPHOUS STEEL

Crystallization kinetics of Fe52Cr18Mo7B16C4Nb3 alloy was evaluated using X-ray diffraction, differential scanning calorimetric (DSC) tests and TEM observations in this research work. In effect, crystallization and growth mechanisms were investigated using DSC tests in four different heating rates (10, 20, 30, 40 K/min) and kinetic models (i.e. Kissinger- Starink, Ozawa, and Matusita methods). ...

متن کامل

Kinetics of Mg6Ni nanocrystallization in amorphous Mg83Ni17

A comprehensive crystallization kinetics study was carried out in order to understand the mechanism of formation of a Mg-rich nanocrystalline Mg6Ni phase in a metallic glass with similar overall composition, Mg83Ni17. Adequate description of the transformation kinetics was obtained by the JMKA equation with an integer Avrami exponent n = 4, associated with nucleation and three-dimensional linea...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Research Letters

سال: 2014

ISSN: 2166-3831

DOI: 10.1080/21663831.2014.911778