Role of Electrolyte Oxidation and Difluorophosphoric Acid Generation in Crossover and Capacity Fade in Lithium Ion Batteries

نویسندگان

چکیده

Poor cycling performance for many high voltage lithium ion batteries (LIB) has been attributed to damage of the anode solid electrolyte interphase (SEI) resulting from crossover reactions. Transition-metal proposed as a primary source SEI and capacity loss, especially high-voltage spinel cathodes. However, deposition transition metals on may not be degradation. This investigation focuses oxidative decomposition LiPF6 in ethylene carbonate (EC)-based electrolytes generate acidic species which subsequently cross over degrade components. The generation strong acid, difluorophosphoric acid (F2PO2H), quantified both graphite || LiNi0.5Mn1.5O4 LiMn2O4 cells. There is correlation between concentration F2PO2H, degradation, loss

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Studies on capacity fade of lithium-ion batteries

The capacity fade of Sony 18650S Li-ion cells has been analyzed using cyclic voltammetry, impedance spectroscopy and electron Ž . Ž . Ž . probe microscopic analysis EPMA . The surface resistance at both the positive LiCoO and negative carbon electrodes were found to 2 increase with cycling. This increase in resistance contributes to decreased capacity. Impedance data reveal that the interfacial...

متن کامل

Electrolyte and Solid-Electrolyte Interphase Layer in Lithium-Ion Batteries

The supply and the management of the energy are particularly at the centre of our daily concerns and represent a socio-economic priority. Indeed, while cars use fossil fuel as the main source of energy for over a century, the depletion of the oil reserves and the necessity to reduce the carbon dioxide emissions, stimulate the development of electric vehicles. Therefore, one of the main challeng...

متن کامل

role of cultural iran in promotion of multilaieralism in central asia and caucasus

cultural iran is a scope that is more extended than the political territories of iran as a political unit. this concept means that cultural geography(mehdi moghanlo-1383-1) of iran is greater than its political geography which, according to history, has a long history extending west-east from kandahar to the euphrates and north-south from the persian gulf to the caucasus including transoxiana a...

15 صفحه اول

Capacity Fade Analysis of Sulfur Cathodes in Lithium–Sulfur Batteries

Rechargeable lithium-sulfur (Li-S) batteries are receiving ever-increasing attention due to their high theoretical energy density and inexpensive raw sulfur materials. However, their rapid capacity fade has been one of the key barriers for their further improvement. It is well accepted that the major degradation mechanisms of S-cathodes include low electrical conductivity of S and sulfides, pre...

متن کامل

Parameter Estimation and Capacity Fade Analysis of Lithium-Ion Batteries Using Reformulated Models

Lithium-Ion Batteries Using Reformulated Models Venkatasailanathan Ramadesigan,* Kejia Chen, Nancy A. Burns, Vijayasekaran Boovaragavan,** Richard D. Braatz, and Venkat R. Subramanian** Department of Energy, Environmental and Chemical Engineering, Washington University, St. Louis, Missouri 63130, USA Department of Chemical and Biomolecular Engineering, University of Illinois, Urbana, Illinois 6...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: ACS energy letters

سال: 2021

ISSN: ['2380-8195']

DOI: https://doi.org/10.1021/acsenergylett.1c01657