Targeted Single-Site MOF Node Modification: Trivalent Metal Loading via Atomic Layer Deposition
Postsynthetic functionalization of metal organic frameworks (MOFs) enables the controlled, high-density incorporation of new atoms on a crystallographically precise framework. Leveraging the broad palette of known atomic layer deposition (ALD) chemistries, ALD in MOFs (AIM) is one such targeted approach to construct diverse, highly functional, fewatom clusters. We here demonstrate the saturatin...
متن کاملMetal-Insulator-Metal Single Electron Transistors with Tunnel Barriers Prepared by Atomic Layer Deposition
Single electron transistors are nanoscale electron devices that require thin, high-quality tunnel barriers to operate and have potential applications in sensing, metrology and beyond-CMOS computing schemes. Given that atomic layer deposition is used to form CMOS gate stacks with low trap densities and excellent thickness control, it is well-suited as a technique to form a variety of tunnel barr...
متن کاملceramic surface modification of textiles by atomic layer deposition
24 Nanoscale ceramic surface modification of textiles by atomic layer deposition R ecent opportunities to merge traditional inorganic materials processing with organic fibrous textiles are creating new possibilities in electrical, optical and mechanical applications for textiles. Textiles are made of low-cost natural or synthetic fibers and have unique flexibility, strength and durability with ...
متن کاملAtomic Layer Deposition of Model Metal Oxide Electrode Architectures
A thorough knowledge of chemical and electrochemical processes that occur at the electrode interface is paramount to the development of improved materials for electrochemical energy storage. One approach is to study model systems with well-defined structures and geometries (architectures) more amenable to systematic and careful study of such materials. The goal of this work is to develop new ap...
متن کاملAtomic Layer Deposition of Noble Metal Thin Films
3 Preface 4 List of publications 5 List of symbols and abbreviations 6
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Chemistry of Materials
سال: 2015
ISSN: 0897-4756,1520-5002
DOI: 10.1021/acs.chemmater.5b01560