Tensile behaviour and fractography analyses of LM6/ZrO2 composites

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Fractography of Polymer Composites: Current Status and Future Issues

With the increasing prevalence of polymer composites in engineering applications, invariably mechanical failures of these components are occurring. Key to addressing this is fractographic analysis; the examination of fracture surfaces to deduce information about the damage and failure of components. The fractography of isotropic materials, particularly metals, has been used as a tool for many y...

متن کامل

Synergetic Use of Thermal and Acoustic Emission in Studying Tensile Behaviour of Fibre Reinforced Composites

The possibility to combine the use of acoustic emission and thermal emission as real-time monitoring techniques on carbon-epoxy composites is the subject of this paper. Tensile tests are therefore performed, using a cross-head speed not too high so to enable a reliable detection of acoustic emission signals, but suitable also for the needs of the thermal emission technique,. The latter techniqu...

متن کامل

Tensile Behaviour and Fracture Characteristics of Polydimethylsiloxane (PDMS) filled Silica Composites

The focus of this study is to investigate the mechanical properties and fracture behaviour of polydimethylsiloxane filled crystalline silica composites (PDMSJCS) via tensile test. The PDMSICS composites were fabricated by using casting method and cured at room temperature for 24 hours. Crystalline silica were filled into PDMS at composition of 2, 6, 10 wt%. The tensile properties of PDMS/2wt%CS...

متن کامل

Effect of Chemical Treatments on Flax Fibre Reinforced Polypropylene Composites on Tensile and Dome Forming Behaviour

Tensile tests were performed on two different natural fibre composites (same constituent material, similar fibre fraction and thickness but different weave structure) to determine changes in mechanical properties caused by various aqueous chemical treatments and whether any permanent changes remain on drying. Scanning electronic microscopic examinations suggested that flax fibres and the flax/p...

متن کامل

Tensile Strength Analysis of bamboo and Layered Laminate Bamboo composites

Tensile properties of bamboo laminae, prepared from bamboo slivers, selected from different regions of bamboo culms (Dendrocalamus strictus), increases from inner to outer region for any cross section and the same is experienced from bottom to top. Application of rule of mixture, on linear regression line drawn from test results, show that fiber strength increases and matrix strength decreases ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materiali in tehnologije

سال: 2017

ISSN: 1580-2949,1580-3414

DOI: 10.17222/mit.2015.319