The aim of the laboratory study was to evaluate the degree of conversion (DC) and surface hardness of two nanofilled resin composite restorative materials compared to three other tooth-colored restorative materials. A light-emitting diode curing unit was used to photo-activate a hybrid composite (FiltekTM Z250), two nanofilled composites (Tetric® EvoCeram, FiltekTM Supreme XT), a nano-ionomer (KetacTM N100) and a compomer (Dyract® eXtra). After 24 hours dry storage in the dark at 37°C, the DC was determined using Fourier transformation infrared spectroscopy (FTIR). A microhardness tester was used to measure the Vickers Hardness Number (VHN). Data for DC and VHN were analyzed using one-way analysis of variance with Tukey’s multiple comparison test, and by using Pearson’s correlation test (P = 0.05 for statistical significance). The highest mean value for DC was obtained with Tetric EvoCeram (79.4 ± 6.7%). Filtek Z250 showed a significantly lower mean DC (58.3 ± 1.8%) than any of the other tested materials (P <0.001). Filtek Supreme XT, Ketac N100, Dyract eXtra and Tetric EvoCeram showed no significant DC differences among them (P >0.05). Filtek Z250 had the highest VHN (97.6 ± 2.8 MPa), while the lowest value was recorded with Tetric EvoCeram (55.3 ± 2.9 MPa). The VHN was significantly different among all tested materials (P <0.001). A significant and highly negative correlation existed between the DC and surface hardness (r = 0.736, P <0.01). The study concluded that Nanofilled composites may have a higher DC and a reduced VHN compared to hybrid composites, with clinical implications. Correlation between these two properties for various nanofilled materials requires further investigation.

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A comparative study of the effects of QTH and LED light curing units on the surface hardness of colored compomer and Hybrid composites

Introduction: One factor affecting the degree of polymerization is the type of light-curing device. The aim of this study was to compare the effects of LED and QTH light curing units on the surface hardness of composite and compomer. Materials & Methods: In this experimental study, 30 samples of composite and compomer were divided into 3 groups of 10 each. One-half of the subgroups in each g...

متن کامل

The Effect of Aging on Nano-Hardness and Modulus of Elasticity of Four Types of Composites: An in-vitro Study

Introduction: Resin composites are an important part of restorative treatment in modern dentistry. There are many trademarks available in Iran market and physico-chemical properties of many of these resin composites are not evaluated yet. This study was carried out to evaluate the physico-chemical properties of four available resin composites and also to assess the effect of aging on their prop...

متن کامل

Surface Roughness of Restorative Materials after Tooth Whitening

Thisin vitro study was conducted to evaluate the effect of tooth whitening on the surface roughness of dental restorative materials using AFM. Two hybrid resin composites and nano-ionomer were fabricated in samples with 2 mm thickness and 6 mm diameter. No changes in roughness was observed for all three materials tested after 14 days of bleaching with 20% carbamide peroxide (CP), compared to th...

متن کامل

Comparative Evaluation of Surface Hardness of Different Resin-Modified Glass Ionomers and a Compomer

Introdouction: Due to the practical problems and time restriction issues in treating dental problems in children, there is a noticeable demand for the application of a convenient handling restorative material with acceptable physical-mechanical properties. The aim of this investigation was to evaluate Vickers microhardness of four tooth-colored restorative materials as a determining mechanical...

متن کامل

بررسی اثر نوع فیلر بر سایش سه جزئی کامپوزیت دندانی

Statement of Problem: The relatively poor wear resistance of dental composite in stress bearing posterior situations has restricted wider clinical application of this restorative material. Purpose: The aim of this study was to evaluate the three body abrasive wear of a dental composite based on a new filler (leucite: KAl Si2O6) and to compare it with the wear resistance of a composite based on ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

ثبت نام

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

عنوان ژورنال:

دوره   شماره 

صفحات  -

تاریخ انتشار 2011