Austenite Stability during Nanoindentation of Ultrafine and Coarse Grained AISI 304L Stainless Steels
نویسندگان
چکیده مقاله:
In the present study, the effect of grain size on the austenite stability was studied by nanoindentation tests in a 304L stainless steel. Thermomechanical processing based on cold rolling and annealing was used to produce two different types of austenite: ultrafine grained (UFG) austenite with the average grain size of 0.65 μm and coarse grained (CG) austenite with the average grain size of 12 μm. Scanning Electron Microscope (SEM) and Transmission Electron Microscope (TEM) were used to follow the microstructural changes during rolling and annealing. The results of nanoindentation tests showed popin in the load-displacement curve of the CG sample while no observable pop-in was found in the UFG sample. The slope of (P/h) versus h plot, where P was load and h was displacement, was changed after the occurrence of each pop-in event in the CG sample. This behavior was related to the change of plastic deformation mode due to the martensitic transformation. The present results, therefore, confirmed that the UFG austenite had higher stability to withstand martensitic transformation.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
austenite stability during nanoindentation of ultrafine and coarse grained aisi 304l stainless steels
in the present study, the effect of grain size on the austenite stability was studied by nanoindentationtests in a 304l stainless steel. thermomechanical processing based on cold rolling and annealing wasused to produce two different types of austenite: ultrafine grained (ufg) austenite with the averagegrain size of 0.65 μm and coarse grained (cg) austenite with the average grain size of 12 μm....
متن کاملMartensitic Transformation in Ultrafine-Grained Stainless Steel AISI 304L Under Monotonic and Cyclic Loading
The monotonic and cyclic deformation behavior of ultrafine-grained metastable austenitic steel AISI 304L, produced by severe plastic deformation, was investigated. Under monotonic loading, the martensitic phase transformation in the ultrafine-grained state is strongly favored. Under cyclic loading, the martensitic transformation behavior is similar to the coarse-grained condition, but the cycli...
متن کاملMartensite phase reversion-induced nano/ ultrafine grained AISI 304L stainless steel with magnificent mechanical properties
Austenitic stainless steels are extensively used in various applications requiring good corrosion resistance and formability. In the current study, the formation of nano/ ultrafine grained austenitic microstructure in a microalloyed AISI 304L stainless steel was investigated by the advanced thermomechanical process of reversion of strain-induced martensite. For this purpose, samples were subjec...
متن کاملmartensite phase reversion-induced nano/ ultrafine grained aisi 304l stainless steel with magnificent mechanical properties
austenitic stainless steels are extensively used in various applications requiring good corrosion resistance and formability. in the current study, the formation of nano/ ultrafine grained austenitic microstructure in a microalloyed aisi 304l stainless steel was investigated by the advanced thermomechanical process of reversion of strain-induced martensite. for this purpose, samples were subjec...
متن کاملMicrostructure and Mechanical Properties of Cold Rolled AISI 304L and 316L Austenitic Stainless Steels during Reversion Annealing
Microstructural evolutions during annealing of cold rolled AISI 304L and AISI 316L stainless steels were studied. Cold rolled AISI 304L alloy was fully martensitic but cold rolled AISI 316L alloy was partially martensitic due to the higher stability of the austenite phase in the latter. During continuous heating to elevated temperatures, the complete reversion of strain-induced martensite at 75...
متن کاملTransient liquid phase bonding of AISI 304L stainless steels with the austenitic and martensitic microstructures
In the present study, the effect of time and base metal microstructure on the Transient Liquid Phase (TLP) bonding of 304L stainless steel was studied. TLP was performed at 1050 0C for 5 and 60 minutes on the coarse grain austenitic and martensitic microstructure using BNi-2 interlayer. To prepare martensitic microstructure, as-received 304L was rolled at -15 0C up to 80% rolling reduction. TEM...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 11 شماره 2
صفحات 1- 5
تاریخ انتشار 2014-06-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023