Effect of welding parameters on pitting corrosion rate of pulsed current micro plasma arc welded AISI 304L sheets in 1N HCl

نویسندگان

  • Chalamalasetti Srinivasa Rao Associate Professor, Department of Mechanical Engineering, AU College of Engineering, Andhra University, Visakhapatnam, India
  • Damera Nageswara Rao Vice Chancellor, Centurion University of Technology & Management, Odisha, India
  • Kondapalli Siva Prasad Assistant Professor, Department of Mechanical Engineering, Anil Neerukonda Institute of Technology & Sciences , Visakhapatnam, India
چکیده مقاله:

Austenitic stainless steel sheets have gained wide acceptance in the fabrication of components, which require high temperature resistance and corrosion resistance such as metal bellows used in expansion joints in aircraft, aerospace and petroleum industries. In the case of single pass welding of thinner sections of this alloy, Pulsed Current Micro Plasma Arc Welding (PCMPAW) has been found beneficial due to its advantages over the conventional continuous current process. This paper highlighted development of empirical mathematical equations using multiple regression analysis, correlating various process parameters to pitting corrosion rates in PCMPAW of AISI 304L sheets in 1 Normal HCl. The experiments were conducted based on a five factor, five level central composite rotatable design matrix. The model adequacy was checked by Analysis of Variance (ANOVA). The main effects and interaction effects of the welding process parameters on pitting corrosion rates of the welded joints were studied using surface and contour plots. From the contour plots, it was understood that peak current was the most influencing factor on the pitting corrosion rate. The optimum pitting corrosion rate was achieved at peak current of 6 Amperes, base current of 4 Amperes, pulse rate of 40 pulses/second and pulse width of 50 % . 

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

effect of welding parameters on pitting corrosion rate of pulsed current micro plasma arc welded aisi 304l sheets in 1n hcl

austenitic stainless steel sheets have gained wide acceptance in the fabrication of components, which require high temperature resistance and corrosion resistance such as metal bellows used in expansion joints in aircraft, aerospace and petroleum industries. in the case of single pass welding of thinner sections of this alloy, pulsed current micro plasma arc welding (pcmpaw) has been found bene...

متن کامل

application of grey relational analysis for optimizing weld pool geometry parameters of pulsed current micro plasma arc welded aisi 304l stainless steel sheets

pulsed current plasma arc welding (pcpaw) is one of the most widely used welding processes in sheet metal manufacturing industry. in any fusion arc welding process, the weld bead geometry plays an important role in determining the mechanical properties of the weld and hence quality of the weld.  moreover, the geometry of weld bead involves several simultaneously multiple quality characteristics...

متن کامل

A study on the effect of pulsed current gas tungsten arc welding parameters on the microstructural evolutions, corrosion behavior and mechanical properties of AA 5456 weld joints

Nowadays, aluminum and its alloys have extensive applications in marine and aerospace industrious owing to their excellent properties. Among these alloys, 5xxx series of aluminum alloys have also excellent corrosion resistance, high toughness and strength and also good weldability. Decrease in yield strength and also tensile strength due to the grain growth in the heat affected zone is of the m...

متن کامل

A study on the effect of pulsed current gas tungsten arc welding parameters on the microstructural evolutions, corrosion behavior and mechanical properties of AA 5456 weld joints

Nowadays, aluminum and its alloys have extensive applications in marine and aerospace industrious owing to their excellent properties. Among these alloys, 5xxx series of aluminum alloys have also excellent corrosion resistance, high toughness and strength and also good weldability. Decrease in yield strength and also tensile strength due to the grain growth in the heat affected zone is of the m...

متن کامل

Effect of Crystallographic Orientation on the Pitting Corrosion Resistance of Laser Surface Melted AISI 304L Austenitic Stainless Steel

The localized corrosion behavior of laser surface melted 304L austenitic stainless steel was studied by potentiodynamic polarization test. The extent of improvement in corrosion resistance was governed by the preferred orientation and the percentage of delta ferrite present on the surface of the laser melted sample. It was established by orientation imaging microscopy that the highest pitting p...

متن کامل

: the effect of sericin levels (silk glue protein) on rate of in vitro maturation, fertilization and culture of sheep oocytes

هدف از آزمایش اول بررسی اثر سطوح مختلف سریسین [0 (control), 0.1, 0.5, 1.0, 2.5 %] افزوده شده به محیط , ivm بر cumulus cell expansion، بلوغ هسته و توسعه متوالی جنین، در گوسفندان نژاد سنجابی در فصل تولید مثلی می باشد. از سرگیری میوز به وسیله خارج شدن اولین پولار بادی اندازه گیری و هم چنین درصد رسیدن جنین های دو سلولی به مرحله کلیواژ و بلاستوسیت نیز به عنوان نشانه ای از میزان شایستگی توسعه اولیه ج...

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 3  شماره 1

صفحات  1- 11

تاریخ انتشار 2013-09-11