Fractographic Aspects of Stress Corrosion Failure of Zircaloy 2 in CH3OH HCL Solutions
نویسنده
چکیده مقاله:
Fracture surface of Zircaloy-2 specimens tested under constant crosshead speed in CH3OH/0.4 Vol. %HCI solution with and without selenium (25 ppm) addition was studied. Using a combined process of deformation and annealing, coarse grained material was also obtained and examined. Two modes of stress corrosion crack propagation were observed: an intergranular zone caused by stress assisted anodic dissolution, and a transgranular cleavage zone, due to hydrogen absorption.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
The Role of Cathodic Poisons on the Stress Corrosion Cracking of Zircaloy- 2 in Methanolic Solution Containing 0.4vol.% Hydrochloric Acid
متن کامل
The Role of Cathodic Poisons on the Stress Corrosion Cracking of Zircaloy- 2 in Methanolic Solution Containing 0.4vol.% Hydrochloric Acid
متن کامل
AN INVESTIGATION ON CORROSION BEHAVIOUR OF A356-10 VOL.% SiC COMPOSITES IN HCl SOLUTIONS
In this study, corrosion behaviour of A356-10 vol.% SiC composites casted by gravity and squeeze casting is evaluated. For this purpose, prepared samples were immersed in HCl solution for 1h at open circuit potential. Tafel polarization and electrochemical impedance spectroscopy (EIS) were carried out to study the corrosion resistance of composites. The Tafel polarization and EIS studies of ...
متن کاملthe role of cathodic poisons on the stress corrosion cracking of zircaloy- 2 in methanolic solution containing 0.4vol.% hydrochloric acid
0
متن کاملINHIBITION OF CORROSION OF CARBON STEEL IN HCl SOLUTIONS BY VARIOUS SCHIFF BASE
Evaluation of corrosion inhibitors for steel in acidic media is important for some industrial facilities as well as is very interesting from theoretical aspects. Most of the effective inhibitors are organic compounds containing nitrogen, phosphorus and sulphur in their structures [1, 2]. Heteroatoms such as nitrogen, oxygen and sulphur are capable of forming coordinate covalent bond with metal ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 3 شماره 1
صفحات 23- 30
تاریخ انتشار 1990-05-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023