Hot Deformation Behavior of Ni80A Superalloy During Non-Isothermal Side Pressing
نویسندگان
چکیده مقاله:
In the present study, the microstructural changes of a Nickel based superalloy Nimonic80A during a non-isothermal deformation were studied. Therefore, microstructure evolutionduring hot side pressing test was predicted with combined methods of finite element analysis andprocessing map of the material. The predicted results were validated through experimentalmicrostructural studies. The results show that the distribution of deformation parameters (i.e.strain, strain rate, and temperature) is non-uniform in the deformed samples. The severity of thisnon-uniformity depends on the amount of sample reduction. High reduction value at one stepforging can cause flow localization and non-uniform dynamic recrystallization, which results theformation of adiabatic shear bands, while using the lower reduction value at each forging step,leads to more uniformly distribution of the deformation parameters and thus uniform the dynamicrecrystallization with the stable flow. Hence the workability and microstructure of the Nimonic80A alloy are mainly depends on the deformation path.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
hot deformation behavior of ni80a superalloy during non-isothermal side pressing
in the present study, the microstructural changes of a nickel based superalloy nimonic80a during a non-isothermal deformation were studied. therefore, microstructure evolutionduring hot side pressing test was predicted with combined methods of finite element analysis andprocessing map of the material. the predicted results were validated through experimentalmicrostructural studies. the results ...
متن کاملHot Deformation Behavior and Pulse Current Auxiliary Isothermal Forging of Hot Pressing Sintering TiAl Based Alloys
This paper focuses on the fabrication of as-forged Ti46.5Al2Cr1.8Nb-(W, B) alloy via pulse current auxiliary isothermal forging (PCIF). The starting material composed of near gamma (NG) microstructure was fabricated by adopting pre-alloyed powders via hot pressing sintering (HPS) at 1300 °C. Isothermal compression tests were conducted at a strain rate range of 0.001-0.1 s-1 and a temperature ra...
متن کاملPrediction of the Hot Compressive Deformation Behavior for Superalloy Nimonic 80A by BP-ANN Model
Abstract: In order to predict hot deformation behavior of superalloy nimonic 80A, a back-propagational artificial neural network (BP-ANN) and strain-dependent Arrhenius-type model were established based on the experimental data from isothermal compression tests on a Gleeble-3500 thermo-mechanical simulator at temperatures ranging of 1050–1250 ̋C, strain rates ranging of 0.01–10.0 s ́1. A comparis...
متن کاملEffects of Carbon on the Microstructure and Hot Deformation Behavior
The effects of carbon content on the dynamic and static softening mechanisms of Ti microalloy steels were investigated both in ferrite and austenite regions. 
The results obtained showed that recrystallization rate decreased as the percentage of carbon content was increased from 0.0035 to 0.110. This is due to the Ti(CN) and TiC precipitates and also the free carbon content. In the ferrite r...
متن کاملEffects of Carbon on the Microstructure and Hot Deformation Behavior
The effects of carbon content on the dynamic and static softening mechanisms of Ti microalloy steels were investigated both in ferrite and austenite regions. The results obtained showed that recrystallization rate decreased as the percentage of carbon content was increased from 0.0035 to 0.110. This is due to the Ti(CN) and TiC precipitates and also the free carbon content. In the ferrite reg...
متن کاملMicrostructural Evaluation of Ti-6AL-4V Alloy during Hot Deformation
Among the titanium alloys, Ti-6Al-4V is the most widely used. In the present work, the uniaxial hot compressive behavior of Ti-6Al-4V has been investigated under constant strain rates. A series of dilatometery experiments were carried out to determine the transformation temperatures at different cooling rates. Specimens were homogenized at 1050 °C for 10 minutes followed by fast cooling to dif...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 2 شماره 1
صفحات 18- 29
تاریخ انتشار 2015-04-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023