Life Estimate of a Compressor Blade through Fractography
نویسندگان
چکیده مقاله:
Failure analysis of fractured components provides some information about the causes and conditions of fracture. Fractography is an indispensable part of the failure analysis as it is usually the only means by which the failure mechanism can be established. By using fractography, some information such as component’s life, values of the stress intensity factor and the applied stress can be calculated. In this paper, the results of categorized investigations and tests such as chemical analysis and fractography of a failed compressor blade of a Frame 6 type gas turbine engine have been presented. The results showed that the source of initial cracks on the blade is corrosion pitting on the surface of the blade. The failure mechanism is high cycle fatigue. Crack growth rate has been calculated from striation spacing and has been compared with the numerical solution. The stress intensity factor range and the applied stress range have also been calculated and compared with numerical results. Fractographic analysis and numerical computations are consistent with each other.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
An Investigation of the Effective Factors in the Shape Rolling Process of a Compressor Blade
One of the most popular forming processes is the shape rolling process in which the desired shape change is achieved by pressing two rollers with a special shape in the opposite rotational direction. In order to improve the product’s quality and reduce production costs, accurate analysis of the shape rolling process of the compressor blades as well as the investigation of the effective paramete...
متن کاملPresenting Three Design Methods for Axial Compressor Blade via Optimization
Improving the efficiency of compressors has been one of the most important goals of researchers over the years. In this paper, three different methods are presented for parameterization and blade optimization of axial flow compressor. All methods consist of flow analysis tool, optimization algorithms, and parametric geometry generation tool, that are different in each approach. Objective functi...
متن کاملExperimental Estimate of Helical Inducer Blade Force
An attachment of inducer is a powerful method to improve the cavitation performance of a turbo-pump. Cavitation surge phenomena, occurring under the severe suction pressure at a partial flow rate, is focused in the present paper. Flow measurements were carried out at the inlet and outlet sections of a flat-plate helical inducer with the solidity of 2.0 and tip blade angle of 11o by using a tota...
متن کاملAreal parametric characterisation of ex-service compressor blade leading edges
In-service the degradation of compressor blade leading edges can have a disproportional effect on compressor efficiency. The high surface curvature in this region makes quantifying the surface finish of this sensitive and prominent region difficult. An automated technique that characterises the roughness of the leading edge in terms of areal parameters is presented. A set of ex-service blades o...
متن کاملLubrication Characteristics Between Bush And Blade Of Swing Compressor
This paper presents the lubrication characteristics between a bush and a blade of a swing compressor that was developed for a new type of compressor for an air conditioner using alternative refrigerants. The mixed lubrication analysis that simultaneously solved the motion equations of the bush and the blade, the lubrication equation and the rough surface contact equation was performed. Moreover...
متن کاملEffect of blade profile on the performance characteristics of axial compressor in design condition
The choice of geometrical shape of the blades has a considerable effect on aerodynamic performance and flow characteristics in axial compressors. In this paper, the effects of the blades shape on the aerodynamic design characteristics are investigated based on Streamline Curvature Method (SCM). Initially, the Streamline Curvature Method (SCM) is used for designing a two-stage axial compressor. ...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 26 شماره 4
صفحات 393- 400
تاریخ انتشار 2013-04-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
کلمات کلیدی
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023