MICROSTRUCTURE, HARDNESS AND SURFACE ROUGHNESS CHARACTERIZATION OF EBM FABRICATED Ti-6Al-4V SAMPLES

نویسندگان

  • Mohammadi, A. Department of Materials Engineering, Isfahan University of Technology, Isfahan 84156-83111, Iran
  • Niroumand, B. Department of Materials Engineering, Isfahan University of Technology, Isfahan 84156-83111, Iran
  • Saboori, A. Department of Applied Science and Technology, Politecnico Di Torino, Torino24, 10129, Italy
چکیده مقاله:

Electron beam melting (EBM) is among the modern additive manufacturing processes whereby metal powders are selectively melted to produce very complicated components with superior mechanical properties. In this study, microstructure, hardness, and surface roughness of EBM fabricated Ti6Al4V samples were characterized. The results showed that the microstructure consisted of epitaxially-grown primary columnar β phase transformed to basketweave and Widmanstatten-type α phase during the subsequent rapid cooling. Martensitic needle-type α phase was also observed on the surfaces of the specimens. It was shown that higher parts of the sample had finer microstructures than the lower parts reaching to less than 340 nm in average thickness of the α layers due to distancing from the hot build platform rendering less opportunity for diffusional β → α+β transformation. The porosity content of the samples was lower than that of some other additive manufacturing processes. Vickers micro-hardness of the samples was measured to be around 337 HV which was higher than those reported for other additive manufacturing processes of the alloy.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Gas-Diffusion Oxynitriding on Microstructure and Hardness of Ti-6Al-4V Alloys

The commercially available titanium alloy, Ti-6Al-4V, was oxynitrided in the deoxygenated nitrogen gas at high temperatures followed by cooling in oxygen-containing nitrogen in order to analyze the influence of oxynitriding parameters on the phase modification, hardness, and the microstructural evolution of the oxynitrided coating. The surface microhardness of the oxynitrided alloy increased du...

متن کامل

Fabrication and characterization of the Ti-6Al-4V/Mg scaffold

Ti–6Al–4V scaffolds were fabricated by powder metallurgical space holder technique in this research. The most added magnesium (Mg) powder was evaporated and a skeleton of Ti-6Al-4V alloy was produced. For this purpose Ti-6Al-4V and Mg powders mixture compacted in a steel die by applying uniaxial pressure of 500 MPa before sintering the green product in a sealed quartz tubes at 900 °C for 2 hour...

متن کامل

Fatigue of Ti-6Al-4V

Metallic biomaterials have essentially three fields of use; these are the artificial hip joints, screw, plates and nails for internal fixation of fractures, and dental implants. Any of these devices must support high mechanical load and resistance of material against breakage is essential. High mechanical properties are needed for structural efficiency of surgical and dental implants. But their...

متن کامل

Optimizing the EDM Parameters to Improve the Surface Roughness of Titanium Alloy (Ti-6AL-4V)

The purpose of this paper is to optimize the EDM parameters to get the better surface finish on the Titanium alloys Ti6AL4V. The continuous advancement of the alloy is fulfilling the demand of the industry but for advance material like Titanium alloys Ti6AL4V partially adopted by industries cause of the difficulties in machining. Non Conventional machining process like Spark Erosion Electrical ...

متن کامل

Ti-6Al-4V triply periodic minimal surface structures for bone implants fabricated via selective laser melting.

Triply periodic minimal surface (TPMS) structures have already been shown to be a versatile source of biomorphic scaffold designs. Therefore, in this work, Ti-6Al-4V Gyroid and Diamond TPMS lattices having an interconnected high porosity of 80-95% and pore sizes in the range of 560-1600 μm and 480-1450 μm respectively were manufactured by selective laser melting (SLM) for bone implants. The man...

متن کامل

Process Mapping, Fracture and Fatigue Behavior of Ti-6al-4v Produced by Ebm Additive Manufacturing

The present work was conducted as part of a larger America Makes funded project to begin to examine the effects of changes in process variables on the resulting microstructure and fracture and fatigue behavior of as-deposited Ti-6Al-4V. In addition to presenting initial results on process mapping of the electron beam powder bed process, the present work also documents the location-dependent pro...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ذخیره در منابع من قبلا به منابع من ذحیره شده

{@ msg_add @}


عنوان ژورنال

دوره 40  شماره None

صفحات  51- 67

تاریخ انتشار 2022-03

با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.

کلمات کلیدی

کلمات کلیدی برای این مقاله ارائه نشده است

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023