Study of Pitting Corrosion Inhibition of Mild Steel by Nitrite in Concrete Pore Solution by Polarization and Zero Resistance Ammetery (ZRA) Techniques (RESEARCH NOTE)
نویسندگان
چکیده مقاله:
A research on the corrosion inhibition of mild steel pitting corrosion in concrete pore solution by sodium nitrite was carried out by employing potentiodynamic, potentiostatic polarization and zero resistance ammetery (ZRA) techniques. Passivity breakdown potential was decreased from the transpassive potential of 700 mV at the absence of chloride to a value of -50 mV when just 0.01M NaCl was added to the test solution and further a decrease to -350 mV was recorded when the concentration of chloride was increased to 0.5M. Addition of NaNO2 into the saturated Ca(OH)2 solution containing 0.5M NaCl considerably shifted the pitting potential towards noble values. Similar results of inhibitive effect of nitrite were obtained from couple potential and current measurement between two nominal identical electrodes through ZRA establishment. In the test solution containing NaNO2, continuous increasing of the corrosion potential towards noble values and simultaneous decrease in couple current density towards zero proved the stability and improvement of the passive film. Whereas, continuous decrease in couple potential accompanied with sharp increase in couple current density with a stable value of 3µA/cm2 at the absence of NaNO2 demonstrated the occurrence of pitting corrosion.
Download for Free
Sign up for free to access the full text
Sign up - It's Free!اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید
ورودمنابع مشابه
SYNERGISTIC INFLUENCE OF NITRITE ON INHIBITION OF MILD STEEL CORROSION IN CHLORIDE CONTAMINATED ALKALINE SOLUTION
Corrosion behavior of mild steel in chloride contaminated alkaline solution has been studied for the period up to 100days. Saturated Calcium hydroxide solution was used as alkaline solution and 0.5M NaCl solution was used to accelerate mild steel corrosion. The Charge transfer resistance Rct, Current density Icorr and inhibition efficiency values were obtained from tafel polarization and electr...
متن کاملCorrosion Inhibition of Mild Steel in Acidic Solution by Apricot Gum as a Green Inhibitor
The inhibitive effect of apricot gum AG on mild steel in 0.5 M phosphoric acid solution was investigated by potentiodynamic polarization, electrochemical impedance spectroscopy EIS, linear polarization resistance and electrochemical noise EN techniques. The inhibition efficiency increased with increasing AG concentration up to a certain value and decreased with increasing temperature. Polarizat...
متن کاملInhibition of Mild Steel Corrosion in Sulfuric Acid Solution by 2-Hydropyrimidine-2-Thione Derivative
The corrosion inhibition potential and efficacy of 2-hydropyrimidine-2-thione derivative on mildsteel in 0.5 M sulfuric acid solution was investigated using electrochemical polarization and FTIRspectroscopic techniques. In addition, docking studies were carried out as theoretical investigationof adsorption inhibitor on iron surface. The results of polarization studies indicate...
متن کاملa genre analytic study of research papers written by bilingual writers and their beliefs: a case of persian-english writers
تحقیق حاضر گزارشی است از تحلیل بخش مقدمه دو دسته از مقالات که عبارتند از: 11 مقاله از دو نویسنده دوزبانه فارسی زبان, که شامل مقدمه 4 مقاله به زبان انگلیسی و چاپ شده در مجلات بین المللی, مقدمه 3 مقاله به زبان انگلیسی و 4 مقاله به زبان فارسی چاپ شده در مجلات داخلی می شود؛ و 12 مقاله از محققان خارجی که در مجله applied linguistics به چاپ رسیده است. مبنای تئوری این تحلیل ها نظریه سوئلز (1990) یا هما...
15 صفحه اولstudy of cohesive devices in the textbook of english for the students of apsychology by rastegarpour
this study investigates the cohesive devices used in the textbook of english for the students of psychology. the research questions and hypotheses in the present study are based on what frequency and distribution of grammatical and lexical cohesive devices are. then, to answer the questions all grammatical and lexical cohesive devices in reading comprehension passages from 6 units of 21units th...
Pitting Corrosion Behaviour of New Corrosion-Resistant Reinforcement Bars in Chloride-Containing Concrete Pore Solution
In this study, the pitting behaviour of a new corrosion-resistant alloy steel (CR) is compared to that of low-carbon steel (LC) in a simulated concrete pore solution with a chloride concentration of 5 mol/L. The electrochemical behaviour of the bars was characterised using linear polarisation resistance (LPR) and electrochemical impedance spectroscopy (EIS). The pitting profiles were detected b...
متن کاملمنابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ذخیره در منابع من قبلا به منابع من ذحیره شده{@ msg_add @}
عنوان ژورنال
دوره 22 شماره 4
صفحات 369- 380
تاریخ انتشار 2009-12-01
با دنبال کردن یک ژورنال هنگامی که شماره جدید این ژورنال منتشر می شود به شما از طریق ایمیل اطلاع داده می شود.
میزبانی شده توسط پلتفرم ابری doprax.com
copyright © 2015-2023