Journal: :journal of lasers in medical sciences 0
merve çakirbay taniş dental practitioner, ankara,turkey turgut cihan akçaboy department of prosthodontics, faculty of dentistry, gazi university, ankara, turkey

introduction: resin cements are generally preferred for cementation of zirconia ceramics. resin bonding of zirconia ceramics cannot be done with the same methods of traditional ceramics because zirconia is a silica-free material. in recent years, many methods have been reported in the literature to provide the resin bonding of zirconia ceramics. the purpose of this in vitro study is to evaluate...

Background and Aim: The aim of this study was to investigate the shear bond strengthof composite to Emax porcelain using different methods of ceramic surface preparation (in vitro). Material and Methods: In this laboratory study, 36 porcelain disks were made and divided into four equal groups. The first group was prepared by sandblasting with 50 micron alumina particles, in the second group rec...

Background and purpose: Bracket debonding is a major problem during orthodontic treatment. This research aimed at studying shear bond strength (SBS) and adhesive remnant index (ARI) in two bonding systems (Assure Plus (adhesion booster) and control). Materials and methods: In this vitro trial, premolars (n=90) were divided into two groups. The brackets were bonded either with Transbond XT or A...

Journal: :Dental materials journal 2007
Makiha Hioki Akikazu Shin-Ya Rizako Nakahara Pekka K Vallittu Yuji Nakasone Akiyoshi Shin-Ya

The objective of this study was to evaluate the influences of enamel shape and bracket base configuration on shear bond strength from a biomechanical point of view. To this end, shear bond test and stress analysis using finite element method (FEM) were performed. Results obtained from both tests were then comprehensively investigated. Maxillary incisors were prepared for plane specimens, while ...

Journal: :journal of dentistry, tehran university of medical sciences 0
m h hosseini assisstant professor, department of orthodontic, school of dentistry, tehran university of medical science, tehran, iran. f namvar j chalipa k saber n chiniforush s sarmadi

the purpose of this study was to compare shear bond strength (sbs) of orthodontic brackets bonded to enamel prepared by er:yag laser with two different powers and conventional acid-etching.forty-five human premolars extracted for orthodontic purposes were randomly assigned to three groups based on conditioning method: group 1- conventional etching with 37% phosphoric acid; group 2- irradiation ...

Journal: :journal of dental school, shahid beheshti university of medical sciences 0
آزیتا کاویانی a kaviani dental school, jondi shapour university of medical sciences, ahvaz-iran.دانشکده دندانپزشکی، دانشگاه علوم پزشکی اهواز نغمه قاری زاده n gharizadeh dental school, jondi shapour university of medical sciences, ahvaz-iran.دانشکده دندانپزشکی، دانشگاه علوم پزشکی اهواز هنگامه علی نژاد h alinejad dental school, jondi shapour university of medical sciences, ahvaz-iran.دانشکده دندانپزشکی، دانشگاه علوم پزشکی اهواز ریحانه موسوی r moosavi

objective: repair of an indirect restoration is usually preferred over its replacement. this study aimed to evaluate the effect of silane in different surface preparation techniques on the bond strength of direct to indirect composite resin.   methods: for this in vitro experimental study, 48 indirect composite cubes were fabricated, divided into 4 groups of 12 and subjected to the following pr...

Journal: :journal of lasers in medical sciences 0
maría vicente prieto dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain ana luisa caseiro gomes dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain javier montero martín contracted professor, dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain alfonso alvarado lorenzo contracted professor, dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain vicente seoane mato dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain alberto albaladejo martínez contracted professor, dental clinic (faculty of medicine), university of salamanca. paseo universidad de coimbra, s/n, 37007, salamanca, spain

introduction: when aesthetics is compromised, dental ceramics are excellent materials for dental restorations; owing to their optical properties and biocompatibility, zirconia ceramics are particularly interesting. self-adhesive resin cements are the most suitable for bonding to zirconia ceramics, but traditional adhesive chemistry is ineffective and surface treatments are required to improve t...

ژورنال: مجله دندانپزشکی 2005
ملکان, الهه , یاسینی, اسماعیل ,

Statement of Problem: The use of dentine bondings on enamel and dentin in total etch protocols has recently become popular. Unfilled resin is hydrophobic and dentin bonding is hydrophilic in nature. This chemical difference could be effective in enamel bonding process. Purpose: The aim of this study was to compare the shear bond strength of unfilled resin to dry enamel and dentin bonding to dry...

A Kaviani, H Alinejad, N Gharizadeh, R Moosavi,

  Objective: Repair of an indirect restoration is usually preferred over its replacement. This study aimed to evaluate the effect of silane in different surface preparation techniques on the bond strength of direct to indirect composite resin.   Methods: For this in vitro experimental study, 48 indirect composite cubes were fabricated, divided into 4 groups of 12 and subjected to the following ...

Alireza Boruziniat Mahshid Gifani, Monavar Nasirzadeh, Mostafa Babazadeh

Aim: To determine the effect of different concentrations and application times of tannic acid on bond strength to dentin. Materials and Methods: Occlusal surfaces of 180 human molars were randomly divided into two groups of immediate shear bond strength evaluation and evaluation after 2 months of storage in collagenase solution. Each group was divided into 10 subgroups according to the solution...