نتایج جستجو برای: ti if steel

تعداد نتایج: 807422  

2009
aniel J. Jorgensen David C. Dunand

Ti–6Al–4V powder preforms containing parallel layers of steel wiremeshes are sintered into composites. Elongatedmacropores are created by electrochemical dissolution of the steel wires, and equiaxedmicroccepted 17 August 2009

Motahari, Poria, Nekoofar, Mohammad hossein, Sharifian, Mohammad reza, Tavakoli, Azadeh,

A comparison of transportation and time of canal preparation with stainless steel hand instruments and Ni-Ti rotary systems (In – Vitro) Dr. MR. Sharifian* - Dr. MH. Nekoofar* - Dr. P. Motahari** - Dr. A. Tavakoli*** *-Assistant Professor of Endodontics Dept. – Faculty of Dentistry – Tehran University of Medical Sciences. **- Assistant Professor of Oral and Maxillofacial Pathology Dept. – Facul...

2016
Anton S. Tremsin Supriyo Ganguly Sonia M. Meco Goncalo R. Pardal Takenao Shinohara W. Bruce Feller

A nondestructive study of the internal structure and compositional gradient of dissimilar metal-alloy welds through energy-resolved neutron imaging is described in this paper. The ability of neutrons to penetrate thick metal objects (up to several cm) provides a unique possibility to examine samples which are opaque to other conventional techniques. The presence of Bragg edges in the measured n...

2013
Tahereh Hosseinzadeh Nik Tabassom Hooshmand Habibeh Farazdaghi Arash Mehrabi Elham S Emadian Razavi

BACKGROUND The purpose of this study was to assess the surface characterization and frictional resistance between stainless steel brackets and two types of orthodontic wires made of stainless steel and nickel-titanium alloys after immersion in a chlorhexidine-containing prophylactic agent. METHODS Stainless steel orthodontic brackets with either stainless steel (SS) or heat-activated nickel-t...

Journal: :Journal of functional biomaterials 2015
Yan Zhou Luke A Perkins Guodong Wang Dongsheng Zhou Hong Liang

Internal fixations provide fast healing but their failure remains problematic to patients. Here, we report an experimental study in failure of three typical cases of metals: a bent intramedullary stainless steel nail, a broken exterior pure Ti plate, and a broken intramedullary stainless steel nail. Characterization of the bent nail indicates that those metals are vulnerable to corrosion with t...

2013
E. G. Zemtsova

This paper presents the scientific rationale for the use of a new generation of functionally graded nano-(L = 50-500 nm) based on the Al-N, Ti-N, Ti-C, Al-O and Mo-S nanolayers (l = 1-10nm) on steel to improve durability for operation in extreme operating conditions of parts and units of machines and mechanisms

2016
Kazuhiro Imai Sachiko Hiromoto

Bulk metallic glasses (BMGs) show higher strength and lower Young's modulus than Ti-6Al-4V alloy and SUS 316L stainless steel. This study aimed to perform in vivo evaluations of Zr65Al7.5Ni10Cu17.5 BMGs for osteosynthesis devices. In the study for intramedullary implants, osteotomies of the femoral bones were performed in male Wistar rats and were stabilized with Zr65Al7.5Ni10Cu17.5 BMGs, Ti-6A...

2007
Masafumi Morita Tokiko Hashimoto Kiyoshi Yamauchi Yuji Suto Takayuki Homma Yuji Kimura

This study was conducted to evaluate the biocompatibility of titanium-nickel shape memory alloy used as a medical implant material. The authors carried out the following electrochemical corrosion test and in vivo and in vitro biological tests for the alloy and some metal and alloys clinically used previously to compare the intensities concerned with the biological reactions, that is, (1) anodic...

Laboratory hot torsion testing technique was carried out on one plain low carbon steel and two plain low carbon Nb and Nb-Ti micro alloyed steels to study the effects of chemical composition, micro alloying addition, on the dynamic softening and grain refinement of ferrite during warm deformation. Deformation schedule was conducted within two phase region (i.e. between Ar3-Ar1). The physical pr...

Journal: :international journal of iron & steel society of iran 2012
m. akbarzadeh a. shafyei h. r. salimijazi

in this study, physical vapor deposition (pvd) ti-cr-n coatings were deposited at two different temperatures100 and 400ºc on hardened and tempered tool steel substrates. the influence of the applied deposition temperature on the physical and mechanical properties of coatings such as roughness, thickness, phase composition, hardness and young’s modulus were evaluated. phase compositions were stu...